ABS Grade A, B, D and E Shipbuilding Steel Plate Explained

What ABS Grade A, B, D and E Have in Common

ABS Grade A, B, D and E are ordinary-strength hull structural steel plates approved under the rules of the American Bureau of Shipping. All four are carbon-manganese steels with exactly the same minimum strength level, and the real difference between them is toughness rather than strength: each grade is qualified by a Charpy V-notch impact test at a progressively lower temperature.

Because the static strength requirement is identical, the choice between A, B, D and E is driven by the service temperature of the part, the plate thickness and the position in the hull, as set out in the classification rules and the approved construction drawings.

Grade Designation and Impact Temperature

Grade Impact test temperature Typical use
A Impact testing generally not required Internal structure and parts in moderate service temperature
B 0 °C Hull and deck structure for temperate service
D -20 °C Hull and deck structure for low-temperature service
E -40 °C Hull structure for the coldest service, exposed decks and northern routes

Mechanical Properties and Chemistry

Ordinary-strength grades share one property band. The values below are minimum requirements; the classification rules reduce them for very thick plate and for plate used in specific locations.

Property Grade A, B, D, E
Yield strength, min 235 MPa
Tensile strength 400-520 MPa
Elongation, min 22 % for thickness up to 50 mm
Impact test Charpy V-notch, temperature according to grade

Chemical composition

ABS ordinary-strength grades are carbon-manganese steels produced to fine-grain, fully killed practice. The rules limit carbon, phosphorus and sulphur and control the manganese range for each grade and thickness.

C: 0.21 % max

Mn: within the range specified by the rules for each grade and thickness

Si: 0.10-0.50 %

P: 0.035 % max

S: 0.035 % max

Als: minimum content required when fully killed fine-grain steel is specified

How the Four Grades Differ in Service

Grade A is approved without impact testing for ordinary temperatures. It is the economical choice for internal bulkheads, non-exposed structure and superstructures in temperate service.

Grade B is impact tested at 0 °C and is widely used for side shell and deck plating of vessels trading in temperate climates.

Grade D is impact tested at -20 °C and is specified for hull and deck structure of vessels that trade in colder waters.

Grade E is impact tested at -40 °C and is reserved for hull structure, exposed decks and other parts required to stay tough at very low sea temperatures.

The rules also raise the required toughness class as plate thickness increases, so a thicker plate in the same location is often ordered in a higher letter grade.

Testing, Certification and Inspection

Unit certification by the classification society, together with mill test certificates to EN 10204 3.1 or 3.2

Heat and lot testing with Charpy V-notch impact specimens taken in the required direction

Ultrasonic examination to ASTM A435, ASTM A577 or ASTM A578 where the order specifies it

Dimensional, marking and surface inspection of every plate

Plate marking with grade, heat number and society approval marks

Optional thickness-direction testing, shot blasting and priming where downstream fabrication requires it

FAQ

Q: Do ABS Grades A, B, D and E have different yield strengths?
No. All four are ordinary-strength hull grades with the same 235 MPa minimum yield strength and the same 400-520 MPa tensile band. They differ in the temperature at which impact toughness is verified.

Q: What is the difference between Grade A and Grade E plate?
Grade A is approved without impact testing for moderate service temperatures, while Grade E must be impact tested at -40 °C and is used where low-temperature toughness is essential.

Q: Was the 480-620 MPa tensile strength quoted for Grade B correct?
No. Figures in that range belong to the high-strength AH32 family, not to ordinary-strength Grades A, B, D and E, which are all specified at 400-520 MPa.

Q: Can Grade B be substituted for Grade A?
In many positions the higher impact class is acceptable because strength is identical, but any substitution must be approved by the classification society and the designer before it is used.

Q: What does the letter H mean in AH32, DH32, EH32 and FH32?
Those are high-strength hull grades with a 315 MPa minimum yield strength. In that family the leading letter again records the impact temperature: A at 0 °C, D at -20 °C, E at -40 °C and F at -60 °C.

Q: What certificates are supplied with the plate?
Mill test certificates to EN 10204 3.1 or 3.2, impact test records for the required temperature, and the classification society's unit certification are normally issued with each heat.