LR Grade EH50 is an extra-high-strength, normalized steel plate for shipbuilding that is approved by Lloyd's Register (LR) and used in marine and offshore structures. It is designed for use in harsh environments and has a minimum yield strength of 500MPa and a tensile strength between 610 and 770 MPa.
The "E" denotes that it has a low-temperature impact toughness of−40∘𝐶, while "H" indicates it is a high-strength grade and "50" signifies a minimum yield strength of 500 MPa.
LR Grade EH50 Shipbuilding Steel Plate Chemical Composition and Mechanical Property
|
LR/EH50 extra high Strength Chemical Composition |
|||||||
|
Grade |
The Element Max (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al |
N |
|
|
LR/EH50 |
0.20 |
0.55 |
1.70 |
0.030 |
0.030 |
0.015 |
0.020 |
|
Nb |
V |
Ti |
Cu |
Cr |
Ni |
Mo |
|
|
0.02-0.05 |
0.03-0.10 |
0.02 |
|
|
|
|
|
|
LR/EH50 extra high strength property |
|||||||
|
Grade |
|
Mechanical Property |
Charpy V Impact Test |
||||
|
Thickness |
Yield |
Tensile |
Elongation |
Degree |
Energy 1 |
Energy 2 |
|
|
LR/EH50 |
mm |
Min Mpa |
Mpa |
Min % |
-40 |
J |
J |
|
t≤50 |
500 |
610-770 |
18% |
33 |
50 |
||
|
50<t≤70 |
500 |
610-770 |
18% |
33 |
50 |
||
|
70<t≤100 |
500 |
610-770 |
18% |
33 |
50 |
||
Key features of LR Grade EH50

Strength:
It is classified as an "extra-high-strength" steel, with a minimum yield strength of 500MPa and a tensile strength of 610–770MPa.
Toughness:
The "E" in the grade indicates it is designed for low-temperature applications, with a specified impact toughness at −20∘𝐶.
Classification:
The steel is certified by Lloyd's Register (LR) for use in shipbuilding and offshore projects.
Application:
It is primarily used in shipbuilding and for marine offshore structures, especially where high strength and low-temperature toughness are required.
Comparison with other grades
Grade EH50 vs. Grade AH50:
EH50 offers enhanced low-temperature toughness, making it suitable for more extreme conditions than AH50.
Grade EH50 vs. Grade E:
EH50 is an extra-high-strength steel, whereas Grade E is a general-strength steel with lower mechanical properties (yield strength of 235MPa and tensile strength of 400-520MPa).
Additional Condition
UT(Ultrasonic examination), AR(As Hot Rolled only), TMCP(Thermal Mechanical Control Processing), N(Normalized), Q+T(Quenched and Tempered),Z Direction Test(Z15,Z25,Z35), Charpy V-Notch Impact Test, The Third Party Test (such as SGS Test), Coated or Shot Blasting and Painting.
FAQ
Q: What does EH50 stand for?
A: E = impact class at -40 °C, H = high-strength hull steel, 50 = minimum yield strength of 500 MPa (the 50 kgf/mm² class).
Q: What is the difference between EH50 and DH50?
A: Both have YS ≥ 500 MPa; DH50 is impact-tested at -20 °C while EH50 at -40 °C, making EH50 suitable for colder and more demanding service.
Q: Which classification societies certify EH50?
A: EH50-type grades exist in the rules of the major societies (LR, ABS, CCS, DNV, BV, KR, RINA and others); the certificate depends on the society requested.
Q: What delivery condition is EH50 supplied in?
A: Commonly normalized; TMCP and quenched-and-tempered conditions are available by order, with supplementary ultrasonic, Z-direction and impact testing as required.
If you want to learn about or purchase other ship plates from GNEE, you can send an email to info@gneesteels.com. We will be very happy to serve you.
| ABS Steel Plate Grade Supplier | ||||
| General Strength | ABS Grade A | ABS Grade B | ABS Grade D | ABS GradeE |
| High Strength | ABS Grade AH32 | ABS Grade DH32 | ABS Grade EH32 | ABS Grade FH32 |
| ABS Grade AH36 | ABS Grade DH36 | ABS Grade EH36 | ABS Grade FH36 | |
| ABS Grade AH40 | ABS Grade DH40 | ABS Grade EH40 | ABS Grade FH40 | |
| Extra Strength | ABS Grade AQ43 | ABS Grade DQ43 | ABS Grade EQ43 | ABS Grade FQ43 |
| ABS Grade AQ47 | ABS Grade DQ47 | ABS Grade EQ47 | ABS Grade FQ47 | |
| ABS Grade AQ51 | ABS Grade DQ51 | ABS Grade EQ51 | ABS Grade FQ51 | |
| ABS Grade AQ56 | ABS Grade DQ56 | ABS Grade EQ56 | ABS Grade FQ56 | |
| ABS Grade AQ63 | ABS Grade DQ63 | ABS Grade EQ63 | ABS Grade FQ63 | |
| ABS Grade AQ70 | ABS Grade DQ70 | ABS Grade EQ70 | ABS Grade FQ70 | |
| ASTM A131 Grade Supplier | ||||
| Ordinary strength | ASTM A131 Grade A | ASTM A131 Grade B | ASTM A131 Grade D | ASTM A131 Grade E |
| low - temperature toughness | ASTM A131 Grade AH32 | ASTM A131 Grade AH36 | ASTM A131 Grade AH40 | |
| / | ||||
| Medium - low temperature toughness | ASTM A131 Grade DH32 | ASTM A131 Grade DH36 | ASTM A131 Grade DH40 | |
| / | ||||
| Better low - temperature toughness | ASTM A131 Grade EH32 | ASTM A131 Grade EH36 | ASTM A131 Grade EH40 | |
| / | ||||
| Ultra - low temperature toughness | ASTM A131 Grade FH32 | ASTM A131 Grade FH36 | ASTM A131 Grade FH40 | |
| / | ||||
| CCS Steel Plate Grade Supplier | ||||
| General Strength | CCS Grade A | CCS Grade B | CCS Grade D | CCS GradeE |
| High Strength | CCS Grade AH32 | CCS Grade DH32 | CCS Grade EH32 | CCS Grade FH32 |
| CCS Grade AH36 | CCS Grade DH36 | CCS Grade EH36 | CCS Grade FH36 | |
| CCS Grade AH40 | CCS Grade DH40 | CCS Grade EH40 | CCS Grade FH40 | |
| Extra Strength | CCS Grade AQ43 | CCS Grade DQ43 | CCS Grade EQ43 | CCS Grade FQ43 |
| CCS Grade AQ47 | CCS Grade DQ47 | CCS Grade EQ47 | CCS Grade FQ47 | |
| CCS Grade AQ51 | CCS Grade DQ51 | CCS Grade EQ51 | CCS Grade FQ51 | |
| CCS Grade AQ56 | CCS Grade DQ56 | CCS Grade EQ56 | CCS Grade FQ56 | |
| CCS Grade AQ63 | CCS Grade DQ63 | CCS Grade EQ63 | CCS Grade FQ63 | |
| CCS Grade AQ70 | CCS Grade DQ70 | CCS Grade EQ70 | CCS Grade FQ70 | |
| LR Steel Plate Grade Supplier | ||||
| General Strength | LR/A | LR/B | LR/D | LR/E |
| High Strength | LR/AH32 | LR/DH32 | LR/EH32 | LR/FH32 |
| LR/AH36 | LR/DH36 | LR/EH36 | LR/FH36 | |
| LR/AH40 | LR/DH40 | LR/EH40 | LR/FH40 | |
| Extra Strength | LR/AH42 | LR/DH42 | LR/EH42 | LR/FH42 |
| LR/AH46 | LR/DH46 | LR/EH46 | LR/FH46 | |
| LR/AH50 | LR/DH50 | LR/EH50 | LR/FH50 | |
| LR/AH55 | LR/DH55 | LR/EH55 | LR/FH55 | |
| LR/AH62 | LR/DH62 | LR/EH62 | LR/FH62 | |
| LR/AH69 | LR/DH69 | LR/EH69 | LR/FH69 | |