Q355B is a new type of Q345B steel under GB/T1591-2018 low alloy structural steel standard. It is equivalent to Q345B in GB/T1591-2008 version and S355JR in EN 10025-2:2004 version.
Chemical composition(%) comparison of Q345B and Q355B:
| Material | C max. | Si max. | Mn max. | P max. | S max. | Cr max. | Ni max. | Cu max. | N max. | Nb max. | V max. | Ti max. | Mo max. |
| Q345B | 0.20 | 0.50 | 1.70 | 0.035 | 0.035 | 0.30 | 0.50 | 0.30 | 0.012 | 0.07 | 0.15 | 0.20 | 0.10 |
| Q355B | 0.20 | 0.55 | 1.60 | 0.030 | 0.030 | 0.30 | 0.30 | 0.40 | 0.012 | - | - | - | - |
Mechanical properties comparison of Q345B and Q355B steel
| Grade | Yield strength MPa in different thickness mm | ||||||||
| ≤16 | 16-40 | 40-63 | 63-80 | 80-100 | 100-150 | 150-200 | 200-250 | 250-400 | |
| Q345B | ≥345 | ≥335 | ≥325 | ≥315 | ≥305 | ≥285 | ≥275 | ≥265 | - |
| Q355B | ≥355 | ≥345 | ≥335 | ≥325 | ≥315 | ≥295 | ≥285 | ≥275 | - |
| Grade | Tensile strength MPa in different thickness mm | ||||||
| ≤40 | 40-63 | 63-80 | 80-100 | 100-150 | 150-250 | 250-400 | |
| Q345B | 470-630 | 470-630 | 470-630 | 470-630 | 450-600 | 450-600 | - |
| Q355B | 470-630 | 470-630 | 470-630 | 470-630 | 450-600 | 450-600 | - |
GNEE can supply both low alloy steel Q345B and Q355B steel plates with further processing service. Welcome to send us inquiry if you are interested in Q345B plate price.
Email: info@gneesteels.com
Whatsapp (WeChat): +86 15824687445
FAQ
Q: What is material grade Q355B?
A: The Q355B equivalent ASTM material
ASTM A572 Grade 50 is a structural steel with high strength and low alloy content that is widely utilized in structural applications. Both Q355B and ASTM A572 Grade 50 have a minimum yield strength of 355 MPa (50 ksi) and possess similar mechanical properties.
Q: What is the difference between Q345 and Q355B?
A: Q345B and Q355B are two different steels, and their main differences are as follows: Different properties: Q345 is a low-alloy steel, while Q355 is a low-alloy, high-strength structural steel widely used in bridges, vehicles, ships, buildings, pressure vessels, special equipment, and other fields.
Q: What is the difference between A36 and Q355B?
A: A36 and Q355B are both structural steel grades, but A36 is an older American standard (ASTM A36) while Q355B is a newer Chinese standard. Q355B generally offers higher strength and potentially better performance in some applications, particularly where higher yield strength is needed.
Q: What is the Indian standard equivalent of Q355B?
A: India: IS 2062 E350 or IS 8500 FE 570 are Indian standards that can be considered as equivalents to Q355B, commonly used in structural applications in India.
Q: What is the European equivalent of Q355B steel?
A: S355JR steels from European British steel standard BS EN10025-2 low alloy high strength steels. These two steel materials Q355B and S355JR are totally equivalent in chemical composition and mechincal properties from the following comparasion data table.
Q: What is the difference between Q355B and Q235B?
A: Different chemical compositions: Q235B has carbon (C) ≤ 0.22%, manganese (Mn) ≤ 1.4%, silicon (Si) ≤ 0.35%, phosphorus (P) ≤ 0.045%, and sulfur (S) ≤ 0.045%, while Q355B has carbon (C) ≤ 0.20%, manganese (Mn) ≤ 1.70%, silicon (Si) ≤ 0.50%, phosphorus (P) ≤ 0.030%, and sulfur (S) ≤ 0.030%.
Q: What is Q355B equivalent to JIS material?
A: Q355 Equivalent Materials
Q355 can be replaced with equivalent materials, including A572 Grade 50 USA ASTM, Q355 China GB/T, and SPFC 590 Vietnam/Japanese JIS.
| Other steel plate | ||||
| Name | Material | Specification (mm) | Tons | Remark |
| Low Alloy | Q345A, Q345B, Q345C, Q345D, Q345E, Q390, Q420, Q460C, ST52-3, S355J2+N, SS400, SA302GrC, S275NL, 35CrMo | 6 - 350 | 5788.56 | Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection |
| Pressure Vessel Plate | Q245R, Q345R, Q370R, 16MnDR, 09MnNiDR, 15CrMoR, 14Cr1MoR, 12Cr2Mo1R, SA516Gr60, SA516Gr70, SA516Gr485, SA285, SA387Gr11, SA387Gr12, SA387Gr22, P265,P295,P355GH,Q245R(R-HIC),Q345R(R-HIC) | 3 - 300 | 8650 | Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection |
| High-Strength Plate | WH785D/E,Q960D/E, Q890D/E,WH60D/E,WH70B,Q550D,Q590D,Q690D/E | 8 - 120 | 3086.352 | Quenched and tempered |
| Wear-Resistant Plate | NM360, NM400, NM450, NM500 | 6 - 150 | 3866.297 | Quenched and tempered |
| Bridge Plate | Q235qC, Q345qC, Q370qC, Q420qC, Q345qDNH, Q370qDNH, A709 - 50F - 2, A709 - 50T - 2 | 8 - 200 | 2853.621 | Hot rolling, normalized ,hot rolling controlled rolling, quenched and tempered + toughness and brittleness |