Q690D High-Strength Steel Plate: Properties and Weldability

What the Q690D Designation Actually Tells a Buyer

Q690D is a high-strength structural steel plate defined in the Chinese national standard GB/T 1591, the same standard family that covers Q355 and Q460. Every character in the designation carries procurement meaning. The letter Q marks the steel as a structural grade specified by minimum yield strength. The number 690 states that minimum yield strength in megapascals, measured on a standard tensile specimen. The letter D is the quality grade and fixes the Charpy V-notch impact test temperature at minus 20 degrees Celsius together with the minimum absorbed energy that must be achieved at that temperature.

That third character is where most specification errors occur. Q690C requires impact testing at 0 degrees Celsius, Q690D at minus 20 degrees Celsius, and Q690E at minus 40 degrees Celsius. All three share the same nominal strength level, so a quotation that names only "Q690" without a quality grade is incomplete and cannot be accepted against a drawing. For a structure that will operate outdoors in winter, or for a fabrication that will be stress relieved, the difference between C and D is the difference between a compliant plate and a rejected one.

Q690D belongs to the thermomechanically controlled or quenched-and-tempered family of steels rather than to the normalised family. This matters because the mechanical properties are developed by a deliberate rolling and cooling schedule, or by a quench-and-temper cycle, and not simply by chemistry. Two plates with identical ladle analysis can end up with very different toughness if the processing route differs. The mill test certificate therefore has to be read alongside the delivery condition, and any subsequent thermal work by the fabricator has to be assessed against the tempering response of that specific route.

Chemical Composition: Lean Carbon, Micro-Alloyed, Low Impurity

The chemistry of Q690D is built around a simple rule: keep carbon low enough for weldability, keep impurities low enough for toughness, and obtain strength from micro-alloying and processing rather than from carbon content. High-carbon steels of equivalent strength exist, but they demand preheat and post-weld heat treatment regimes that most structural fabrication shops cannot sustain, and they lose toughness in the heat-affected zone.

In practice, carbon for Q690D is normally held at or below about 0.20 percent, with many thermomechanically rolled products delivered considerably lower, in the 0.10 to 0.16 percent band. Silicon sits around 0.15 to 0.60 percent, manganese in the 1.00 to 2.00 percent range depending on the producer and thickness, and phosphorus and sulphur are controlled tightly, typically 0.025 percent and 0.015 percent maximum respectively for the higher quality grades. Niobium, vanadium and titanium are added in small amounts, generally below 0.10 percent each, to pin grain growth and contribute precipitation strengthening. Chromium, molybdenum, nickel and copper may be present as optional alloying elements or as residuals, and their total is restricted so that the carbon equivalent stays within the limits the standard sets for the grade and thickness.

Carbon equivalent is the single most useful chemistry number for the welding engineer. For Q690D, both the CEV formula based on carbon, manganese, chromium, molybdenum, vanadium, nickel and copper, and the Pcm formula used for lower-carbon quenched and tempered steels, are relevant, and the applicable limit depends on thickness and on the delivery condition. A certificate that reports only tensile results and omits carbon equivalent is not sufficient for a welding-critical purchase; ask for the full analysis with the CEV or Pcm value computed.

Parameter Typical Q690D requirement Procurement note
Carbon 0.20% max (often 0.10-0.16%) Lower carbon improves HAZ toughness and reduces preheat demand
Silicon 0.15-0.60% Deoxidation element; excessive Si harms toughness
Manganese 1.00-2.00% Strength and hardenability; raises CEV
Phosphorus 0.025% max Segregation element; tight limits required for D grade
Sulphur 0.015% max Controls inclusion shape and through-thickness ductility
Nb + V + Ti Each typically 0.10% max Grain refinement and precipitation strengthening
Carbon equivalent Per standard, thickness dependent Must be reported on the mill certificate for weldability assessment

Mechanical Property Requirements and the Meaning of Grade D

The headline numbers for Q690D are a minimum yield strength of 690 MPa, a tensile strength range of approximately 770 to 940 MPa, and a minimum elongation after fracture of about 14 percent on a 50 mm gauge length. These are floor values, not targets, and a plate that sits at the floor on elongation while sitting at the ceiling on tensile strength is a less forgiving plate than one with a balanced property profile. Buyers ordering for cold forming should look at the actual elongation reported on the certificate, not only at the yield strength.

Thickness has a direct effect on achievable properties. Because the centre of a thick plate cools more slowly than the surface during quenching, and because the rolling reduction ratio falls as thickness rises, the standard permits the minimum yield strength to step down for greater thicknesses. A 25 mm plate and a 100 mm plate may both be sold as Q690D but will not have the same guaranteed yield strength. The purchase order should state the thickness range explicitly so the mill applies the correct line of the property table.

The D quality grade requires Charpy V-notch impact testing at minus 20 degrees Celsius, with a minimum absorbed energy normally specified at 47 joules for the longitudinal direction on full-size specimens. Two points deserve attention during acceptance. First, the test direction matters: transverse specimens generally give lower absorbed energy than longitudinal ones, so a certificate must state the direction used. Second, sub-size specimens produce lower absolute values and the standard scales the requirement accordingly; comparing a sub-size result directly against a full-size 47 joule criterion is a common inspection error.

Property Q690D specified value Test basis
Minimum yield strength (ReH) 690 MPa for thinner gauges, reduced stepwise as thickness increases Tensile test per GB/T 228.1
Tensile strength (Rm) Approximately 770-940 MPa Tensile test per GB/T 228.1
Elongation after fracture (A) Approximately 14% min 50 mm gauge length
Impact energy at -20 degrees C 47 J min, longitudinal, full-size specimen Charpy V-notch per GB/T 229
Delivery condition TMCP or quenched and tempered Stated on the mill certificate

Delivery Condition and Heat Treatment Routes

Q690D arrives in one of two conditions, and they are not interchangeable in fabrication. Thermomechanically controlled processed plate achieves its strength through controlled rolling in the non-recrystallisation temperature range followed by accelerated cooling. The microstructure is fine-grained and the plate retains relatively low internal stress. Quenched and tempered plate is austenitised, water quenched and then tempered at a temperature chosen to reach the strength and toughness balance. Quenched and tempered plate of this strength class has a tempered martensitic or bainitic structure and responds predictably to a subsequent stress-relief cycle, provided the relief temperature stays below the original tempering temperature.

The practical consequence is that any thermal cycle applied after delivery is a change to the certified condition. Stress relief is often requested for welded assemblies, particularly where machining follows welding or where dimensional stability is critical. A stress-relief treatment for Q690D is normally performed in the 550 to 580 degrees Celsius range with controlled heating and cooling rates, and it must be demonstrated by a procedure qualification that the treatment does not push the tensile strength below the minimum or the impact energy below 47 joules. Mills will state a maximum permitted stress-relief temperature on the certificate for this reason.

Normalising is not a suitable treatment for Q690D. Normalising dissolves the benefit of thermomechanical processing and, for quenched and tempered plate, produces a ferrite-pearlite structure that cannot reach 690 MPa yield. A plate that has been inadvertently normalised, for example by passing through a furnace with a different load, has lost its certification and should be re-qualified or downgraded. Annealing and full quenching from the as-supplied condition are likewise re-manufacturing operations that require a fresh heat treatment procedure and new testing.

Welding Q690D: Preheat, Heat Input and Hydrogen Control

Welding is where a 690 MPa steel earns or loses its certification. Three variables dominate: hydrogen, heat input and restraint. Hydrogen comes from moisture in consumables and on the joint surface; low-hydrogen consumables are mandatory, held in a heated quiver at the correct temperature and used within their permitted exposure window. Cellulosic electrodes and rutile electrodes with high moisture pickup should not be used on this steel.

Preheat is required for most thicknesses and is normally set in the 100 to 150 degrees Celsius range for plate above about 20 mm, with interpass temperature capped to protect toughness. The preheat value should come from the welding procedure qualification for the specific combination of steel grade, thickness and consumable, not from a generic table. Heat input must be controlled within the qualified window: too low a heat input produces hard, crack-susceptible heat-affected zones, while too high a heat input coarsens the grain and reduces impact energy below the 47 joule requirement. A typical qualified window for gas-shielded and submerged arc welding on this grade lies between roughly 10 and 25 kilojoules per centimetre, with t8/5 cooling times monitored on critical joints.

Restraint matters because the yield strength is high. Fit-up should avoid excessive gap and avoid forcing plates into position, since the residual stress locked in by forced fit-up adds directly to the stress that drives hydrogen-assisted cracking. Where full-penetration welds are required, a buttering or a soft root pass technique reduces the risk of cracking in the high-restraint root region. Post-weld heat treatment, when applied, follows the same temperature limits described in the previous section, and the heating and cooling rates should be slow enough to avoid thermal gradients across the assembly.

Consumable matching deserves a deliberate choice rather than a default. Undermatching consumables, with deposited strength somewhat below the base metal, are commonly used on high-strength structural steel to improve toughness and reduce cracking risk, on the understanding that the joint design carries the load. Overmatching consumables raise joint strength but increase hydrogen cracking susceptibility. The welding procedure specification should record the actual deposited composition and strength, and the qualification should include impact testing of the weld metal and the heat-affected zone at minus 20 degrees Celsius to match the parent plate grade.

Forming, Cutting and Machining Considerations

Cold forming of Q690D is possible but limited. The high yield-to-tensile ratio, typically above 0.85 for quenched and tempered plate, leaves little reserve between the onset of yielding and the ultimate strength, so a bend that springs back heavily or a formed part that work-hardens locally can crack on the outside radius. Minimum bend radii for this class are substantially larger than for Q355, and the bend line should ideally run transverse to the rolling direction rather than parallel to it. After cold forming, a stress-relief treatment is advisable if the part will be welded or machined.

Thermal cutting is the normal route for plate of this thickness. Laser and plasma cutting produce a narrow, hard cut edge; that edge is acceptable for most structural work provided the hardness is checked when the joint will be welded without removing the cut face. For fatigue-critical or full-penetration joints, grinding back the cut edge to remove the hardened layer and any dross is standard practice. Oxy-fuel cutting requires preheat on thick sections and produces a wider heat-affected zone, which should be accounted for in the cutting allowance.

Machining follows the same logic as welding: the material is strong and abrasive, so rigid set-ups, sharp carbide tooling and conservative depths of cut are needed. Drilling thin plate without adequate support leads to work hardening under the drill point and rapid tool failure. Where holes are numerous, drilling before the part reaches full hardness, or using a helical milling rather than a pure drilling strategy, gives better tool life and hole quality.

Applications Where Q690D Pays Off, and Where It Does Not

The economic case for Q690D is weight and section reduction. In a mobile structure, whether that is a crane boom, a concrete pump arm, a mining truck body or a trailer chassis, reducing plate thickness by 30 to 40 percent relative to a Q355 design cuts dead weight that the machine has to carry and move. In fixed structures, the benefit is reduced section size where headroom or architectural limits constrain the design. The grade is used for high-rise building transfer structures and heavy columns, for excavator and loader arms, for crane jibs and outriggers, for ship structures requiring high strength in a thin section, and for frames of heavy machinery where stiffness and strength must coexist.

The grade is the wrong choice in three common situations. First, where stiffness governs rather than strength: because Young's modulus is essentially the same for all structural steels at about 206 GPa, replacing Q355 with Q690D does not increase stiffness, and a deflection-limited design will simply become more slender and more prone to buckling. Second, where the plate will be subject to high-cycle fatigue in a poorly detailed joint: higher strength does not raise the fatigue class of a weld detail, which is governed by geometry and weld quality. Third, where the fabrication shop lacks the discipline for preheat, controlled heat input and low-hydrogen handling, since the consequences of a hydrogen crack in a 690 MPa steel are more severe than in a mild steel.

Buckling deserves specific mention because it is the most frequent disappointment. A plate that is thin enough to exploit high yield strength is also thin enough to buckle locally. Design checks for local slenderness, plate buckling and lateral-torsional buckling must be redone against the reduced thickness, and stiffener spacing usually has to be revisited. When the design is converted properly, the weight saving is real; when only the material callout is changed, the structure becomes unsafe.

Inspection, Tolerances and Documentation

Acceptance of Q690D plate rests on three documents and one set of measurements. The mill test certificate must state the grade with quality grade, the delivery condition, the heat number, the plate dimensions, the full chemical analysis including carbon equivalent, the tensile results with yield, tensile and elongation, the Charpy results with test temperature, specimen size and direction, and the maximum permitted stress-relief temperature where applicable. The certificate must be traceable to the plate by marking, and the marking must survive delivery and handling.

Dimensional inspection follows the general plate tolerance framework, with thickness tolerance applied against the ordered nominal thickness and flatness checked over the full plate length. Thickness should be measured at several points on a grid rather than at the centre only, since the crown of a rolled plate is at mid-width. Surface inspection looks for laminations, seams, scale pits and edge cracks; laminations matter more than usual on this grade because through-thickness stress in welded T-joints can open a subsurface discontinuity. Where Z-direction properties are needed, that requirement must be stated at the order stage, since through-thickness tensile testing is not part of the standard delivery scope.

Ultrasonic testing is frequently specified for plate destined for pressure-retaining or dynamically loaded components. The acceptance class should be named in the purchase order, because ultrasonic testing of plate is performed against defined quality classes and an unclassified requirement cannot be adjudicated. Similarly, if the fabricator intends to stress relieve, the order should state the intended relief temperature so the mill can confirm the delivery condition is compatible.

FAQ

Q: What is the difference between Q690D and Q690E?
Both grades share the same minimum yield strength of 690 MPa. The difference is the quality grade letter, which sets the Charpy impact test temperature: D requires testing at minus 20 degrees Celsius, E at minus 40 degrees Celsius. Q690E is specified for colder service and carries a tighter impurity control in practice.

Q: Can Q690D plate be stress relieved after welding?
Yes, provided the stress-relief temperature stays below the original tempering temperature of the plate and a procedure qualification confirms that tensile strength and impact energy remain above the specified minima afterwards. A range of 550 to 580 degrees Celsius is typical, with controlled heating and cooling rates.

Q: Why does the minimum yield strength of Q690D decrease for thick plate?
Because thicker sections cool more slowly at the centre during accelerated cooling or quenching and receive less rolling reduction, the achieved strength is lower. GB/T 1591 therefore applies a thickness-dependent property table, and the purchase order must state the gauge so the correct line is used.

Q: Is normalising acceptable for Q690D?
No. Normalising destroys the microstructure responsible for the strength and, for quenched and tempered plate, produces a ferrite-pearlite structure that cannot reach 690 MPa yield. Plate that has been normalised loses its certification and must be re-tested or downgraded.

Q: What consumables should be used to weld Q690D?
Low-hydrogen consumables matched or slightly undermatching the base metal strength, stored and handled under controlled conditions. The welding procedure qualification should include weld metal and heat-affected zone impact testing at minus 20 degrees Celsius to align with the parent plate grade.

Q: Does Q690D improve fatigue performance compared with Q355?
Not directly. Fatigue strength of welded details is governed by joint geometry, weld toe profile and flaw size rather than by base metal yield strength. Higher strength helps only where the detail is smooth and the stress range is fully elastic, and it makes the structure more sensitive to stress concentrations.

Q: How is Q690D plate thickness verified on receipt?
By measuring on a grid across the plate rather than at a single point, because rolled plate is thicker at mid-width. Measurements are compared against the nominal thickness and the applicable tolerance for the ordered width and length, and results should be recorded against the heat number.