Dec 22, 2025 Leave a message

S690QL-QUALITY-CERTIFICATE.pdf

What grade is S690QL steel material?

 

General Introduction

 

 

ASTM 690 (S690QL) is a high-strength structural steel grade specified under EN 10025-6, supplied in a quenched and tempered (Q&T) condition. It is engineered for load-bearing structures requiring exceptional strength, reliable toughness, and controlled weldability, particularly in demanding and safety-critical environments.

 

ASTM 690

 

Through a carefully balanced alloy design-primarily carbon, manganese, silicon, and controlled additions of chromium, molybdenum, and vanadium-S690QL delivers a unique combination of high yield strength, fracture resistance, and structural stability.

 

 

Comprehensive Performance Overview

 

 

The defining feature of S690QL steel is its minimum yield strength of 690 MPa, enabling engineers to design thinner, lighter structures without sacrificing safety margins. This directly translates into:

Reduced steel consumption

Lower transportation and installation costs

Improved payload efficiency

In addition, S690QL exhibits reliable low-temperature impact toughness, making it suitable for cold regions and dynamically loaded structures.

 

Key Advantages

High Strength-to-Weight Ratio
Enables lighter designs with equivalent or higher load capacity.

Good Weldability for High-Strength Steel
Compatible with common welding processes when proper preheating is applied.

Excellent Toughness
Maintains structural integrity under impact and low-temperature conditions.

 

Limitations to Consider

Higher Cost
Alloying elements and Q&T processing increase production cost.

Low-Temperature Sensitivity
Extreme cold applications require strict impact testing compliance.

Limited Stock Availability
Compared to conventional grades such as S355.

Historically, S690QL has been widely adopted in heavy machinery, offshore structures, cranes, and high-rise buildings, where structural efficiency and safety are decisive factors.

 

 

Standards, Designations & Equivalent Grades

 

 

Standard Body Grade Region Remarks
EN S690QL Europe Primary reference standard
DIN 1.8928 Germany Equivalent EN designation
ASTM A572 Grade 65 USA Similar strength, lower low-temp toughness
UNS S690QL International Closest global reference
JIS - Japan No direct equivalent

Note: While ASTM A572 Grade 65 offers comparable strength, it generally does not match S690QL's low-temperature impact performance.

 

 

Chemical Composition (Typical)

 

 

Element %
C 0.12 – 0.20
Mn 1.00 – 1.60
Si 0.10 – 0.50
Cr 0.20 – 0.50
Mo 0.10 – 0.30
V 0.02 – 0.10
P ≤ 0.025
S ≤ 0.015

Alloying Element Functions

Carbon: Strength and hardness control

Manganese: Hardenability and toughness

Chromium & Molybdenum: Strength retention and thermal stability

Vanadium: Grain refinement and yield strength enhancement

 

 

Mechanical Properties (Quenched & Tempered)

 

 

Property Typical Value
Yield Strength ≥ 690 MPa (≥ 100 ksi)
Tensile Strength 690 – 770 MPa
Elongation ≥ 20%
Reduction of Area ≥ 50%
Hardness 200 – 250 HB
Charpy V-Notch Impact ≥ 27 J @ -40°C

This balance of strength and ductility ensures excellent resistance to both static and dynamic loading.

 

 

Physical & Thermal Properties

 

 

Property Value
Density 7.85 g/cm³
Melting Point 1420 – 1540 °C
Thermal Conductivity ~50 W/m·K
Specific Heat 0.46 kJ/kg·K

 

 

Corrosion & Heat Resistance

 

 

S690QL offers good atmospheric corrosion resistance, but like most high-strength structural steels, it requires protective coatings in aggressive environments.

Chloride environments: Risk of pitting

Acidic environments: Not recommended without protection

 

Temperature Limits

Continuous service: ≤ 400 °C

Intermittent exposure: ≤ 500 °C

Scaling risk: > 600 °C

 

 

Fabrication Characteristics

 

 

Weldability

S690QL is weldable using standard methods such as MIG, TIG, and SMAW, with recommended preheating to reduce hydrogen cracking risk.

Process Typical Filler
MIG ER70S-6
TIG ER70S-2
SMAW E7018

Machinability

Relative machinability: ~60% (vs AISI 1212 = 100%)

Carbide tooling recommended

Formability

Cold forming: Limited

Hot forming: Preferred for complex shapes

Heat Treatment

Quenching (850–900°C): Strength enhancement

Tempering (500–600°C): Toughness optimization

 

 

Typical Applications

 

 

Industry Application
Construction High-rise buildings
Heavy Machinery Excavators, cranes
Offshore Oil & gas platforms
Transportation Bridges
Others Mining equipment, shipbuilding, pressure vessels

S690QL is selected when structural efficiency, safety margins, and long-term reliability are critical.

 

 

Comparison with Other Grades

 

 

Property S690QL S355 S700MC
Strength High Moderate Very High
Toughness Excellent Good Moderate
Weldability Good Excellent Moderate
Formability Limited Good Moderate
Cost High Moderate High
Availability Limited High Limited

 

S690QL (STE 690) is a premium high-strength quenched and tempered structural steel designed for demanding engineering applications. While its cost and availability require careful planning, its exceptional mechanical performance, toughness, and design efficiency make it a preferred material for critical load-bearing structures.

 

Contact now

 

info-536-393

Q1: What does the designation "S690QL" specifically mean?
A: The designation breaks down as follows:

S: Structural steel.

690: Minimum guaranteed yield strength in MPa (ReH ≥ 690 MPa).

Q: Quenched.

L: Delivered in the quenched and tempered condition.
Therefore, S690QL is a thermomechanically rolled, quenched, and subsequently tempered steel plate, offering an optimal balance of very high strength and good toughness.

Q2: What is the key microstructural advantage of the "QL" (Quenched & Tempered) process?
A: After quenching, which forms a hard but brittle martensitic structure, the steel is tempered (reheated typically between 550-650°C). This tempering process:

Improves Toughness and Ductility: It transforms the brittle martensite into tougher tempered martensite (or bainite), dramatically increasing impact resistance and elongation.

Relieves Internal Stresses.

Provides Stability: The resulting microstructure is stable, offering consistent mechanical properties and superior performance under dynamic and fatigue loading compared to just quenched (Q) grades.

Q3: What are the typical mechanical properties for S690QL according to EN 10025-6?
A:

Yield Strength (ReH): 690 - 890 MPa (minimum 690 MPa).

Tensile Strength (Rm): 770 - 940 MPa.

Elongation (A₅): Typically ≥ 14%.

Impact Toughness (Charpy V-notch): Minimum average of 40 Joules at -40°C (for grade L). Some specifications may require 27J at -60°C (grade L1).

Q4: Why is S690QL considered "readily weldable" despite its very high strength? What are the critical precautions?
A: The tempering treatment improves weldability compared to non-tempered high-strength steels. However, strict procedures are mandatory due to its high carbon equivalent (CET/CEV ~0.40-0.45):

Preheating: Essential to prevent hydrogen-induced cold cracking (HICC). Temperature (often 100-150°C+) depends on thickness, CET, and hydrogen level of the consumable.

Low-Hydrogen Practice: Use only certified low-hydrogen (H5 or H10) welding consumables. Electrodes must be properly baked, and filler wires protected from moisture.

Heat Input Control: Must be maintained within a specified window (e.g., 0.8-1.5 kJ/mm). Too low leads to HAZ hardening; too high can over-temper and soften the HAZ, reducing strength below specification.

Interpass Temperature: Must be controlled, usually with a defined maximum (e.g., 250°C) to prevent microstructural degradation.

Q5: Is Post-Weld Heat Treatment (PWHT) required for S690QL?
A: It is not always mandatory but is highly recommended for thick sections (>30-50mm) and highly restrained joints or for critical applications (e.g., offshore, crane booms). PWHT (e.g., 550-600°C) serves to:

Diffuse residual hydrogen.

Temper the hard martensite in the Heat-Affected Zone (HAZ).

Relieve welding stresses, improving fatigue performance and dimensional stability.
The decision is governed by the applicable fabrication code and design requirements.

Q6: Can I use undermatching or overmatching welding consumables for S690QL?
A: Both are common, with specific purposes:

Undermatching (e.g., 500 MPa filler): Often used to ensure HAZ and weld metal toughness, as softer weld metal can yield and redistribute stress. It requires careful design approval, as the weld itself becomes the strength-limiting factor.

Matching/Overmatching (e.g., 700+ MPa filler): Used when the full strength of the joint must be utilized. This demands extremely precise welding procedures to maintain toughness and avoid cracking. It is common for critical, highly loaded components.

Send Inquiry

whatsapp

phone

Email

Inquiry