Aug 22, 2025 Leave a message

ASTM-A36.pdf

What is the difference between A36 and ST52 steel plate?

A36 and ST52 are both types of carbon steel, but they have different properties and are used in different applications.

 

Here's a detailed comparison of the two:

 

A36 Steel

 

 

 Standard: ASTM A36

info-356-336

 Chemical Composition:

  • Carbon (C): 0.25-0.29%
  • Manganese (Mn): 0.60-0.90%
  • Phosphorus (P): ≤ 0.04%
  • Sulfur (S): ≤ 0.05%
  • Silicon (Si): ≤ 0.40%

 

 Mechanical Properties:

  • Yield Strength: Minimum 250 MPa (36,000 psi)
  • Tensile Strength: 400-550 MPa (58,000-80,000 psi)
  • Elongation: 20-23% in 200 mm (8 inches)

 

 Applications

  • Structural steel used in construction and engineering
  • Commonly used in buildings, bridges, and other infrastructure projects
  • Suitable for welding and forming

 

ST52 Steel

 

 

 Standard: DIN 17100, EN 10025

info-269-365

 Chemical Composition:

  • Carbon (C): ≤ 0.22%
  • Manganese (Mn): 1.60%
  • Phosphorus (P): ≤ 0.045%
  • Sulfur (S): ≤ 0.045%
  • Silicon (Si): ≤ 0.55%

 

 Mechanical Properties:

  • Yield Strength: Minimum 355 MPa (51,500 psi)
  • Tensile Strength: 490-630 MPa (71,000-91,000 psi)
  • Elongation: 22% in 200 mm (8 inches)

 

 Applications:

  • Higher strength steel used in machinery, structural applications, and transportation equipment
  • Often used in manufacturing of heavy machinery, cranes, and mining equipment
  • Suitable for welding, forming, and machining

 

Key Differences

 

 

Strength:

ST52 has a higher yield and tensile strength compared to A36, making it suitable for more demanding applications where higher strength is required.

 

Composition:

A36 has a higher carbon content compared to ST52, while ST52 has higher manganese content which contributes to its strength.

 

Standards:

A36 is an ASTM standard specification in the United States.

ST52 conforms to DIN and EN standards commonly used in Europe.

 

Applications:

A36 is primarily used in construction and structural applications where low to moderate strength is sufficient.

ST52 is used in applications requiring higher strength and better mechanical properties, such as in machinery and heavy equipment.

 

Summary

 

 

While both A36 and ST52 are carbon steels, ST52 is stronger and has better mechanical properties, making it suitable for more demanding applications compared to A36. The choice between the two will depend on the specific requirements of the project, including the required strength, toughness, and standards compliance.

 

Email: info@gneesteels.com
Whatsapp (WeChat) :+86 15824687445

 
FAQ

Q: What is St 52.3 material standard?

A: ST52-3 material or mechanical properties, ST 52.3 material is a low alloy, high power physical steel which can be freely welded to other wieldable steel. ST52-3 steel's Powered properties is Yield power more than 355 MPa, tensile power 490-630Mpa.

Q: What is s152 3 material?

A: Description. ST52-3 grade steel is a readily weldable low carbon manganese steel with good impact resistance (including in sub-zero temperatures). This material is commonly supplied in the untreated or normalised condition. Machinability of this material is similar to that of mild steel.

Q: What is the difference between A36 and ST52-3?

A: Key Differences
ST52 has a higher yield and tensile strength compared to A36, making it suitable for more demanding applications where higher strength is required. Composition: A36 has a higher carbon content compared to ST52, while ST52 has higher manganese content which contributes to its strength.

Q: What is the difference between ST52 and s355?

A: ​​Low-Temperature Toughness​​: S355J2 guarantees impact toughness at ​​-20°C​​, outperforming St52-3 (tested at 0°C). ​​Strength Consistency​​: St52-3 has a higher tensile strength lower bound (490 vs. 470 MPa), ensuring reliability in static load designs.

Q: What is the steel equivalent to the ST52-3?

A: What is the steel grade ST52 equivalent to?
While exact equivalents may vary based on standards and specifications, ST52-3 is commonly compared with S355JR due to similar mechanical properties and applications.

Q: What is DIN 17100 ST52-3 equivalent to?

A: DIN 17100 ST 52.3 equivalent EN steel S355JR offers high yield strength and tensile strength, and it is supplied with a variety of treatments and test options to ensure that it is a highly usable steel in your various projects.

Q:What is A36 Steel Plate?

A: ASTM A36 Steel Plate is one of the most common grades of steel used in structural applications. This mild carbon steel grade contains chemical alloys that give it properties such as machinability, ductility, and strength that are ideal for use in constructing a variety of structures.

Q: What is A36 steel equivalent?

A: The A36 equivalent material grade, ASTM A36 equivalent grades are ASTM A283C, JIS G3101 SS400, JIS G3106 SM400A, EN10025-2 S235JR, DIN17100 ST37-2, FE360B, E24-2, etc.

 

Other steel plate
Name Material Specification (mm) Tons Remark
Low Alloy Q345A, Q345B, Q345C, Q345D, Q345E, Q390, Q420, Q460C, ST52-3, S355J2+N, SS400, SA302GrC, S275NL, 35CrMo 6 - 350 5788.56 Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection
Pressure Vessel Plate Q245R, Q345R, Q370R, 16MnDR, 09MnNiDR, 15CrMoR, 14Cr1MoR, 12Cr2Mo1R, SA516Gr60, SA516Gr70, SA516Gr485, SA285, SA387Gr11, SA387Gr12, SA387Gr22, P265,P295,P355GH,Q245R(R-HIC),Q345R(R-HIC) 3 - 300 8650 Normalizing, tempered ,controlled rolling, hot rolling , Hot rolling,1st inspection, 2nd inspection, 3rd inspection
High-Strength Plate WH785D/E,Q960D/E, Q890D/E,WH60D/E,WH70B,Q550D,Q590D,Q690D/E 8 - 120 3086.352 Quenched and tempered
Wear-Resistant Plate NM360, NM400, NM450, NM500 6 - 150 3866.297 Quenched and tempered
Bridge Plate Q235qC, Q345qC, Q370qC, Q420qC, Q345qDNH, Q370qDNH, A709 - 50F - 2, A709 - 50T - 2 8 - 200 2853.621 Hot rolling, normalized ,hot rolling controlled rolling, quenched and tempered + toughness and brittleness

 

Send Inquiry

whatsapp

phone

Email

Inquiry