What "Ordinary" and "Coloured" Really Describe
In stainless steel trade language, an "ordinary" plate means a mill-finish product whose surface is the natural result of rolling, annealing and pickling or skin-passing: silver-grey, uniform, and with no applied colour layer. A "coloured stainless steel pattern plate" is a composite product: a stainless substrate that has been given both a texture and a colour film, so the visible surface is neither bare metal nor a simple paint layer. Confusing the two leads to wrong specifications, because the properties a buyer cares about in one product are almost irrelevant in the other. On plain plate the governing issues are grade, finish, flatness and thickness tolerance. On coloured pattern plate the governing issues are substrate grade, texture pattern, colour process, film adhesion, colour fastness and how the sheet will be cut and bent without damaging the edge.
The two product families are covered by different parts of the same standards framework. The substrate is ordered to GB/T 3280 for cold-rolled plate, sheet and strip, GB/T 4237 for hot-rolled plate, ASTM A240/A240M, or JIS G 4305, depending on the market. The colour layer is not covered by any of these; it is governed by supplier data sheets and by test methods such as ISO 9227 or ASTM B117 for salt spray, ASTM D3359 for coating adhesion, ASTM D3363 for pencil hardness and ASTM D523 for gloss. Understanding that split is the single most useful thing a buyer can take from this article.
Substrate Grades and Why They Decide the Colour Result
Coloured sheet is normally produced from cold-rolled 304 (UNS S30400), 316L (UNS S31603), 201 or, for cost-sensitive interior work, 430 ferritic. The substrate choice controls two things the colour layer cannot fix: corrosion resistance at cut edges and scratches, and the base reflectivity that shows through a thin PVD or electrochemical film.
Grade 201 is a manganese-bearing austenitic grade with roughly 16-18% Cr, 3.5-5.5% Ni and 5.5-7.5% Mn. It takes colour well and forms readily, but its lower nickel and absence of molybdenum make it noticeably less resistant to chloride staining in humid or coastal interiors, and its higher work-hardening rate means tight bend radii crack more easily. Grade 304 is the mainstream choice for architectural and elevator work: 18-20% Cr, 8-10.5% Ni, adequate for indoor and most urban outdoor exposure when the surface is kept clean. Grade 316L adds 2.0-3.0% Mo and is specified where chlorides, de-icing salts or marine air are present. Grade 430 is ferritic, magnetic and cheap; it accepts colour but has limited bendability and will show rust bloom at cut edges in damp conditions.
For pattern plate the substrate must also be deep-drawing or bending quality, because the embossed pattern is rolled into the surface before colouring and the textured valleys concentrate forming strain. A 201 substrate with a coarse pattern and a 0.6 mm thickness is a common combination for interior wall panels; a 304 substrate at 0.8-1.2 mm is normal for elevator doors and column cladding, where flatness under reflected light is judged by eye.
Mill Finishes on Ordinary Plate: What the Buyer Is Actually Ordering
Plain stainless plate is defined largely by its finish code, and most disputes about "different appearance" trace back to a finish mismatch rather than a grade mismatch.
| Finish | How it is produced | Typical Ra roughness | Typical use |
|---|---|---|---|
| No.1 | Hot rolled, annealed and pickled | Coarse, 2.0-4.0 um | Industrial plate, vessel shells, further processing |
| 2D | Cold rolled, annealed, pickled, dull skin pass | 0.6-1.5 um | Forming stock, parts to be polished later |
| 2B | Cold rolled, annealed, pickled, bright skin pass | 0.2-0.6 um | General purpose, the default for coloured sheet substrate |
| BA | Cold rolled then bright annealed in a controlled atmosphere | 0.05-0.20 um | Highly reflective, appliances, reflective trim |
| No.4 | Ground with a 120-150 grit abrasive | 0.6-1.0 um | Brushed architectural panels, kitchen equipment |
| HL | Hairline, unidirectional abrasive | 0.3-0.6 um | Elevator interiors, appliance fronts |
| No.8 | Mirror polished to a near-specular finish | Below 0.05 um | Decorative mirrors, high-end cladding |
Roughness values are indicative ranges from normal commercial practice rather than fixed limits, and any requirement should be agreed as a measured Ra with a cut-off length, plus a visual master sample under defined lighting. On a coloured product the substrate finish is not cosmetic detail: a 2B substrate under a 0.3-0.5 um PVD film produces a satin colour, while the same colour on a No.8 substrate produces a mirror finish in which every handling mark and fingerprint is visible. That is why mirror-plus-colour sheet is sold with a protective PVC film and why buyers should specify both the substrate finish and the film type.
How the Colour Is Produced: Three Processes with Different Physics
There are three commercial routes, and they behave so differently in service that they should be treated as separate products.
Electrochemical colouring. The stainless surface is treated in a hot chromic-sulphuric acid bath under controlled potential, which thickens the natural passive film into an interference film of a few hundred nanometres. Colour comes from thin-film interference, so the hue depends on film thickness rather than on a pigment: bronze, gold, red, blue, green and black are produced by progressively thicker films. Because the colour is part of the oxide film and not an added layer, it does not peel, and it retains the metallic lustre of the substrate. Its limits are colour consistency across a run, sensitivity to bath chemistry, and a colour that shifts with viewing angle.
PVD coating. Titanium, zirconium or chromium is vaporised in vacuum and reacted with nitrogen or a hydrocarbon to deposit a nitride or carbonitride film roughly 0.2-1.0 um thick. Titanium nitride gives the familiar gold, zirconium nitride a paler brass gold, chromium nitride a dark grey, and titanium carbonitride the black shades used on appliance and elevator trim. PVD films are hard, typically 1500-2500 HV for TiN, and are deposited at low temperature so the substrate keeps its annealed temper. They are also line-of-sight processes, so deep textures can shadow and lose colour in the valleys.
Organic and nano-coating. A clear or pigmented resin, sometimes with nano-ceramic particles, is applied over a textured or coloured surface and cured. This route delivers the widest colour range and the lowest cost, and can be applied to a coil rather than a sheet. It is also the least abrasion resistant and the most susceptible to UV chalking outdoors; on exterior cladding it should be treated as a five-to-ten-year finish, not a permanent one.
Pattern Plate: Embossed, Etched and Checkered Surfaces
"Pattern" in this context covers three distinct textures. Embossed plate is produced by passing the strip between engraved rolls, transferring a raised or recessed design such as a diamond, linen or stucco pattern into the surface; the deformation is metallurgical and permanent, and the pattern depth is typically 0.02-0.10 mm for architectural sheet. Etched plate is produced by applying a resist and attacking the exposed surface with acid, giving a two-tone decorative effect that is often combined with a PVD colour so the recesses read darker. Checkered or tear-drop plate is the industrial version, rolled for slip resistance on floor plate and stair treads, and is normally supplied uncoloured in a No.1 or 2B finish.
The practical consequence of texture is that it hides defects. Fingerprints, minor scratches, waviness and even small dents are far less visible on an embossed surface than on a mirror surface, which is why textured coloured sheet dominates hotel lobby panelling and elevator doors where daily handling is unavoidable. The trade-off is cleanability: a deep pattern traps dust and requires mechanical rather than wipe cleaning, and in food-contact or clinical areas a textured surface is normally disallowed because it cannot be reliably sanitised.
Performance Comparison: What Each Surface Survives
The table below compares plain and coloured surfaces on the properties that generate claims after installation. Values are typical commercial ranges and should be confirmed against the supplier data sheet for the specific product, since process control varies widely between lines.
| Property | Plain 2B / No.4 plate | Electrochemical colour | PVD colour film | Organic / nano coating |
|---|---|---|---|---|
| Film thickness | None | 0.05-0.3 um oxide | 0.2-1.0 um | 2-20 um |
| Surface hardness | Substrate, roughly 200 HV | Similar to substrate | 1500-2500 HV | 2H-4H pencil |
| Neutral salt spray resistance | Grade dependent, no film to lose | Good, colour stable | Very good on 304 substrate | Moderate, edge creep likely |
| UV stability outdoors | Not applicable | Stable, inorganic film | Stable, inorganic film | Limited, chalking and fade |
| Scratch repair | Repolish locally | Difficult, film removal visible | Difficult, film removal visible | Not repairable |
| Weldability | Full | Colour destroyed at weld and heat tint zone | Film destroyed near weld | Film burned back 20-50 mm |
The most common field failure of coloured sheet is not film wear but corrosion creep at cut edges and drilled holes. A sheared edge exposes bare substrate; on a 201 substrate in a humid bathroom or a coastal lobby this appears as a brown stain creeping out from the cut within months. Specifying 304 or 316L substrate for edges that will remain exposed, and sealing or trimming those edges, matters more than the hardness of the colour film.
Fabrication Rules: Form First, Colour Second Where Possible
Colour films do not stretch. Bending a coloured sheet around a tight radius cracks the film on the outside of the bend and shows a bright line, so the sequence should be decided at design stage. Where the design permits, parts should be cut and formed from plain plate and coloured afterwards, particularly for complex pressings. Where the coloured sheet must be formed, the minimum inside bend radius should be at least 2-3 times the thickness for a 0.8 mm PVD sheet and larger for thick organic coatings, with the bend line running parallel to the rolling direction.
Laser cutting is acceptable if the protective film is left on and the assist gas is nitrogen; oxygen cutting and plasma cutting leave a heavy oxide edge that is difficult to clean without damaging the film. Welding is the hardest operation: the heat tint zone must be removed mechanically, and any colour film within 10-30 mm of the weld is destroyed. The usual practice is to weld plain components, finish and polish the weld, and then colour the assembly, or to design the joint so that the weld falls behind a cover profile. Shearing should use a sharp, small-clearance blade to avoid a rolled edge that lifts the film. Protective PVC film should be removed within the supplier's stated window, typically three to six months, because adhesive residues cure under sunlight and become difficult to remove.
Selection Guide by Application
Interior architectural cladding, column covers and reception panelling: 304 substrate at 0.8-1.2 mm, embossed or etched texture, PVD colour, hidden fixings. Elevator car doors and jambs: 304 at 1.0-1.5 mm, hairline or mirror substrate, PVD or electrochemical colour, film-protected through installation. Kitchen splashbacks and appliance fronts: 304 at 0.6-1.0 mm, 2B or No.4 substrate, PVD for abrasion resistance. Exterior signage and canopies: 316L where chlorides are present, electrochemical colour preferred because there is no discrete film to chip. Industrial floor plate and stair treads: plain 304 checkered or tear-drop plate, no colour, since abrasion would destroy any film within weeks.
Where cost is decisive and the environment is dry and interior, 201 substrate with an organic coating is a legitimate choice, provided the specification states the substrate grade on the certificate and the buyer accepts that cut edges will need protection. Substituting 201 for 304 without disclosure is the most frequent quality failure in this product category and is detectable in seconds with a spot test for manganese or with a portable analyser.
Cost Structure: Why the Price Gap Is Not Arbitrary
A coloured pattern plate costs more than a plain plate for reasons that can be itemised, and doing so is the best defence against an offer that looks too low. The substrate carries a premium when a specific finish such as BA or No.8 is required, and a further premium for 304 or 316L over 201. Embossing consumes roll life and adds a separate pass. Colour adds a vacuum or chemical process with its own yield loss: PVD coating lines accept limited coil width, so a 1500 mm wide requirement forces slitting and scrap. Colour matching generates off-spec material at the start and end of a run. Protective film, interleaving paper, wooden crating and edge protection add cost that plain plate does not carry, and international freight on a fragile, scratch-sensitive surface requires better packaging than coil.
When comparing offers, request the same six parameters in writing: substrate grade and its certificate, substrate finish, thickness and tolerance, texture pattern reference, colour process and colour reference sample, and film type. A quotation that omits any of these cannot be compared, because a 20% lower price is usually a 201 substrate, a 2B finish substitution, or an organic coating standing in for PVD. Acceptance testing should include visual comparison against a retained master sample under defined lighting, an adhesion cross-cut test to ASTM D3359, a pencil hardness test to ASTM D3363, and a salt spray test to ISO 9227 or ASTM B117 on a representative panel.
FAQ
Q: Is coloured stainless steel plate simply painted stainless steel?
No. Electrochemical colouring converts the passive film into an interference oxide a few hundred nanometres thick, and PVD deposits a hard nitride film in vacuum. Only the lowest-cost products use an organic paint or resin layer, and those are the ones that fade outdoors.
Q: Can coloured stainless steel plate be welded and still keep its colour?
Not at the joint. Any colour film within roughly 10-30 mm of a weld is destroyed by heat, and the heat tint must be removed mechanically. Components are normally welded in plain condition, finished, and coloured afterwards, or the weld is hidden behind a cover profile.
Q: Why does the colour look different on a mirror finish and on a brushed finish?
Because the film is thin enough to be partly transparent, so the substrate reflectivity shows through. A No.8 mirror substrate gives a saturated, high-gloss colour, while a 2B or hairline substrate gives a softer satin tone of the same nominal colour.
Q: What is the difference between 201 and 304 substrate for coloured sheet?
201 uses manganese instead of part of the nickel, with roughly 16-18% Cr and 3.5-5.5% Ni. It colours and forms adequately but stains at cut edges in humid or coastal conditions, and its higher work-hardening rate makes tight bends prone to cracking.
Q: How long does a PVD colour last outdoors?
The nitride film itself is inorganic and does not fade, and on a 304 or 316L substrate it performs well in urban and inland exterior exposure. Service life is limited instead by substrate corrosion at cut edges and by scratch damage, so edge detailing decides the outcome.
Q: Does a textured pattern plate hide damage better than a plain plate?
Yes. Embossing and etching break up reflected light, so fingerprints, minor scratches and surface waviness are far less visible. The trade-off is that the texture traps dust and cannot be wiped clean as easily, which rules it out of food-contact and clinical areas.