What is the yield strength of ASME SA662 Grade C ?
The minimum yield strength of ASME SA662 Grade C pressure vessel steel plate is 295 MPa (43 ksi). It is a carbon-manganese-silicon steel designed for moderate and lower temperature service with a tensile strength range of 485–620 MPa.

ASME SA662 Grade C is a fabrication-grade steel plate designed for high-quality fusion welding in the manufacture of heavy-duty pressure boundaries. Produced under the strict metallurgical controls of ASME Section II, it is characterized by its high manganese-to-carbon ratio which enhances weldability and reduces the risk of cold cracking in the heat-affected zone (HAZ). Because it is a fully killed, fine-grained steel, it provides a stable response to the intense heat of arc welding, ensuring that the finished welded joints meet the same rigorous toughness standards as the base metal, even in thick-walled sections.
Key Characteristics
Low Carbon Equivalent: Designed to minimize the risk of hydrogen-induced cracking during the welding of pressure boundaries.
Manganese Strengthening: Higher manganese levels (0.85--1.50%) enhance the material's hardenability without the brittle tendencies of high carbon.
Cleanliness (Fully Killed): Produced with minimal impurities (P and S) to prevent hot-cracking and laminations during rolling and fabrication.
PWHT Stability: Retains its mechanical properties and impact toughness even after multiple Post-Weld Heat Treatment (PWHT) cycles.
Grade Designation
ASME: American Society of Mechanical Engineers.
SA: Prefix for Ferrous material specifications.
662: The standard for C-Mn-Si steel for low-temperature service.
Grade C: The high-strength tier within the SA662 specification.
Comparison (vs. SA299 Grade A)
Temperature Target: SA299 is for high-temperature boiler service, whereas SA662 Grade C is for low-to-moderate temperature vessels.
Ductility Comparison: SA662 Grade C is strictly fine-grained for toughness, while SA299 focuses on carbon-based strength for steam drums.
Chemical Philosophy: SA662 Grade C uses manganese for strength; SA299 uses higher carbon levels which can make welding more difficult.
Impact Testing: SA662 Grade C is much more likely to pass mandatory impact testing for sub-zero service than SA299.

Common Application
Boiler Steam Separators: Cylindrical vessels used to separate saturated steam from water in medium-pressure boilers.
Desalination Pressure Chambers: High-pressure shells used in the flash evaporation stage of water desalination.
Nitrogen Storage Units: Pressurized tanks used in food preservation and electronics manufacturing facilities.
Emergency Shutdown (ESD) Accumulators: High-pressure cylinders used to store energy for emergency valve operation.
Chemical Reactor Shells: The primary pressure-retaining shells for reactors in chemical synthesis plants.
What is the impact toughness of ASME SA 662 Grade C?
ASME SA 662 Grade C provides adequate impact toughness at moderate temperatures, making it resistant to brittle fracture under normal operating conditions. However, it is not designed for use in cryogenic applications or environments where extreme temperatures could compromise its toughness. For low-temperature applications, materials like SA 537 or SA 516 with enhanced impact resistance are recommended.
What are the advantages of using ASME SA 662 Grade C in pressure vessel construction?
The main advantage of using ASME SA 662 Grade C in pressure vessel construction is its cost-effectiveness combined with good strength, ductility, and weldability. These properties make it ideal for moderate to high-pressure environments, such as in chemical processing and power generation. Its toughness ensures that it can withstand mechanical stresses, while the material's flexibility allows it to be fabricated into complex shapes for different vessel designs.
What are the limitations of ASME SA 662 Grade C?
While ASME SA 662 Grade C is ideal for moderate-pressure applications, it is not suitable for extreme pressure or high-temperature environments. For applications requiring high-strength materials or those that exceed 800°F (427°C), materials like SA 516 or SA 537 should be considered for improved creep resistance and high-temperature strength.
SA662 Grade C pressure vessel steel chemical composition %
| Grade | C max | Mn | P max | S max | Si max |
| SA662 Grade C | 0.20 | 1.00-1.60 | 0.025 | 0.025 | 0.15-0.40 |
SA662 Grade C pressure vessel steel Mechanical properties
| Class | Tensile strength Rm MPa | Yield strength ReH MPa min | Elongation A% min in | |
| 200mm | 50mm | |||
| SA662 Grade C | 485-620 | 295 | 18 | 22 |
1What industries commonly use ASME SA 662 Grade C?
ASME SA 662 Grade C is used primarily in industries that require pressure vessels and boilers to operate at moderate to high temperatures and pressures. It is commonly found in the chemical, petrochemical, oil & gas, and power generation industries, where its balance of strength and ductility makes it ideal for the fabrication of equipment exposed to mechanical and thermal stresses.
2What is the chemical composition requirements for ASME SA 662 Grade C?
The chemical composition of ASME SA 662 Grade C typically includes Carbon (0.18–0.23%), Manganese (0.60–0.90%), Silicon (0.15–0.40%), Phosphorus (≤ 0.035%), and Sulfur (≤ 0.035%). These elements help ensure a balance of strength, ductility, and weldability, making it suitable for moderate to high-pressure applications in boilers and pressure vessels.
3What are the advantages of using ASME SA 662 Grade C in pressure vessel construction?
The main advantage of using ASME SA 662 Grade C in pressure vessel construction is its cost-effectiveness combined with good strength, ductility, and weldability. These properties make it ideal for moderate to high-pressure environments, such as in chemical processing and power generation. Its toughness ensures that it can withstand mechanical stresses, while the material's flexibility allows it to be fabricated into complex shapes for different vessel designs.
4What is the weldability of ASME SA 662 Grade C?
ASME SA 662 Grade C has good weldability, making it suitable for joining with common welding methods such as SMAW, GTAW, and SAW. However, proper welding procedures and preheating are essential, particularly for thicker sections, to prevent cracking and to maintain the material's integrity after welding.
5What is the maximum temperature limit for ASME SA 662 Grade C?
The maximum temperature limit for ASME SA 662 Grade C is typically around 800°F (427°C). Beyond this temperature, the material may start to lose its strength and become more susceptible to creep. For applications involving higher temperatures, alloys such as SA 516 or SA 204 are more suitable, as they offer better performance under extreme thermal conditions.
6What is the tensile strength of ASME SA 662 Grade C?
The tensile strength of ASME SA 662 Grade C typically ranges from 70 to 90 ksi (485 to 620 MPa). This level of tensile strength makes it suitable for moderate to high-pressure applications. The material can withstand mechanical stress and thermal loads typical in pressure vessels, heat exchangers, and boilers while maintaining its strength without deforming under pressure.
7What is the post-weld heat treatment (PWHT) requirement for ASME SA 662 Grade C?
Yes, post-weld heat treatment (PWHT) is often required for ASME SA 662 Grade C, especially for thicker sections. PWHT helps to relieve residual stresses and improve the material's weldability and toughness. The typical post-weld heat treatment temperature is around 1100–1200°F (593–649°C), depending on the thickness of the material and the specific application requirements.