Why Understanding the Properties of ASTM A516 Grade 70 Is Critical?
ASTM A516 Grade 70 (or ASME SA-516 Gr. 70) is the world's most widely specified carbon steel plate for pressure vessel quality (PVQ) applications. Whether you are designing boilers, fabricating heat exchangers, or erecting storage tanks, this material is almost certainly on your bill of materials. However, simply knowing which grade to select is only half the battle-understanding the engineering significance behind each property is what separates a safe, cost-effective design from a costly oversight.


For procurement teams and engineering managers, asking "What are the primary properties of ASTM A516 Grade 70?" is far from a theoretical exercise. It directly impacts:
- Wall Thickness Calculations ---Yield strength dictates the lower threshold for shell wall thickness reduction.
- Weld Procedure Specification (WPS) --- Carbon equivalent determines preheat requirements and hydrogen control protocols.
- Low-Temperature Suitability--- Charpy V-notch (CVN) impact toughness establishes the minimum design metal temperature (MDMT).
- Material Substitution Decisions --- Precise property data enables confident evaluation of alternative plate grades.
Need A516 Grade 70 plates with guaranteed properties?
GNEE supplies PVQ carbon steel plates with full EN 10204 3.1/3.2 Mill Test Reports - every plate traceable from melt to delivery. Stock thicknesses 5–205mm, normalized condition, third-party inspection available.
ASTM A516 Grade 70 PVQ Carbon Steel Plate Specification
| Parameter | Standard |
|---|---|
| Thickness | 5 – 205 mm |
| Width | 1,500 – 3000 mm |
| Length | 6,000 – 12,000 mm |
| Condition | As-Rolled / Normalized |
| Certification | EN 10204 3.1 MTR |
ASTM A516 Grade 70 PVQ Carbon Steel Plate Chemical Composition
| Thickness | C (max) | Mn | Si | P (max) | S (max) |
|---|---|---|---|---|---|
| ≤ 12.5 mm | 0.27% | 0.85–1.20% | 0.15–0.40% | 0.035% | 0.035% |
| > 12.5 – 50 mm | 0.28% | ||||
| > 50 – 100 mm | 0.30% | ||||
| > 100 – 205 mm | 0.31% |
ASTM A516 Grade 70 PVQ Carbon Steel Plate Mechanical Property
| Property | Grade 70 Value |
|---|---|
| Tensile Strength | 485 – 620 MPa (70 – 90 ksi) |
| Yield Strength (min) | 260 MPa (38 ksi) |
| Elongation (200 mm, min) | 17% |
| Elongation (50 mm, min) | 21% |
| Bend Test | 180° - no fissures |
ASTM A516 Grade 70 carbon steel plate Weldability Properties & Carbon Equivalent
Carbon Equivalent (CEV)
The carbon equivalent condenses the combined effect of carbon and alloying elements into a single weldability indicator. The standard IIW formula is:
CEV Formula (International Institute of Welding):
CEV = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15
Typical A516 Grade 70 CEV by thickness:
≤ 12.5 mm: ~0.40 – 0.43
12.5 – 50 mm: ~0.42 – 0.45
50 – 100 mm: ~0.43 – 0.46
> 100 mm: ~0.44 – 0.48
CEV ≤ 0.40, thickness ≤ 12.5 mm:
Typically requires no preheating (applicable to low-restraint joints).
CEV 0.40–0.45, thickness > 12.5 mm:
Minimum preheat temperature of 10°C (50°F).
CEV > 0.45, thickness > 50 mm:
Minimum preheat temperature of 50–100°C (120–210°F), depending on joint restraint and hydrogen control requirements.
Note: Welding Procedure Specifications (WPS) must always be drafted and qualified in accordance with ASME Section IX or AWS D1.1 for your specific application.
Recommended welding consumables
| Process | Consumable (AWS Classification) | Typical Application |
|---|---|---|
| SMAW (Stick) | E7018 (AWS A5.1) | Field erection, repair, positional welding |
| GMAW (MIG/MAG) | ER70S-6 (AWS A5.18) | Shop fabrication, high deposition |
| FCAW | E71T-1 (AWS A5.20) | Positional welding with good penetration |
| SAW | F7A0-EM12K (AWS A5.17) | Long straight seams, highest deposition |
| GTAW (TIG) | ER70S-2 (AWS A5.18) | Root passes, high-quality welds |
ASTM A516 Grade 70 PVQ plate Heat Treatment & Property Effects
The delivery condition (heat treatment state) of A516 Grade 70 significantly affects its final properties. Understanding these conditions helps buyers specify the right material for their application:
| Condition | Thickness | Process | Property Effect |
|---|---|---|---|
| As-Rolled (AR) | ≤ 12.5 mm (standard) | Hot rolling, no post-rolling HT | Adequate for moderate service; lower toughness |
| Normalized (N) | > 12.5 mm (standard) | 870–910°C, air cool | Refined grain → improved toughness & uniformity |
| Stress Relieved (SR) | Optional, all t | 540–650°C, slow cool | Relieves residual stresses from forming/welding |
| N + SR | Optional, all t | Normalize then stress relieve | Maximum toughness + low residual stress |
Post-Weld Heat Treatment (PWHT) Guidelines:
In accordance with ASME BPVC Section VIII Division 1 (UCS-56), Post-Weld Heat Treatment (PWHT) is mandatory for P-No. 1 Group 2 materials when the nominal weld thickness exceeds 38mm (1.5in.) [or 32mm / 1.25in. depending on specific joint details and exemptions].
PWHT Holding Temperature: 595--650℃ (1100--1200℉).
Holding Time: 1 hour per 25mm (1in.) of thickness.
PWHT restores heat-affected zone (HAZ) toughness and reduces peak residual stresses-critical factors for vessels subject to cyclic loading or operating at sub-ambient temperatures.
Comparison with Other PVQ Grades
Impact test optional (S5).
Impact test included.
Impact test mandatory.
| Comparison | Key Difference | When to Choose |
|---|---|---|
| Gr 70 vs Gr 65 | +35 MPa tensile, +20 MPa yield; −2% elongation | Gr 70 when you need max strength; Gr 65 for balanced performance at lower cost |
| Gr 70 vs A515 Gr 70 | A516: lower Si, better low-temp toughness; A515: higher Si, better elevated-temp strength | A516 for ≤500°F service; A515 for intermediate elevated-temperature applications |
| Gr 70 vs Q345R (GB 713) | Comparable strength but different composition limits, testing protocols, and certification systems | Not direct equivalents - substitution requires engineering approval per applicable code |
| Gr 70 vs P355GH (EN 10028) | Similar tensile level (355 min yield vs 260); European spec has different chemistry and CE marking | Not interchangeable - PED/CE-marked vessels may require P355GH specifically |
ASTM A516 Grade 70 PVQ Carbon Steel Plate Main Applications
Process vessels, separators, surge drums, high-pressure reactors
Boiler shells, steam drums, mud drums in utility and industrial boilers
Refinery vessels, hydrotreaters, separators, production equipment
API 650 and API 620 tanks, LPG vessels, pressurized storage
Shell & tube exchangers, tube sheets, channel heads
- Power plant auxiliaries, feedwater heaters, deaerators
Reactor vessels, columns, accumulators, process piping components
Offshore platform process equipment, FPSO vessels
Flue gas desulfurization, water treatment pressure vessels

GNEE Steel Technical Team
18+ years of pressure vessel steel plate export experience. Our technical team provides material selection guidance, welding procedure recommendations, and full supplementary testing support for ASTM A516, A387, A537, and other PVQ steel grades.
🏭
EN 10204 3.1/3.2 Certified
🔍
SGS · BV · TÜV Inspected
🌍
60+ Countries Served
⏱️
18+ Years PVQ Export
📦
3,000+ Tons Stocked
With 18+ years of PVQ steel export experience, GNEE is trusted by fabricators and EPC contractors in 60+ countries. We provide:
- Stock thicknesses 5–205mm - normalized, with full EN 10204 3.1/3.2 MTR
- Supplementary testing: Charpy (S5), HIC (S8), UT (A578), CEV control (S20)
- Third-party inspection by SGS, BV, TÜV, Lloyd's Register
- Custom cutting, beveling, and surface preparation before shipment
- Global delivery - container and bulk vessel to any port worldwide


Can A516 Grade 70 be used for sour service (H2S)?
Yes, ASTM A516 Grade 70 can be used for sour service containing hydrogen sulfide (H₂S), but only if it is specially ordered, processed, and tested to meet sour service requirements. Standard off-the-shelf A516 Grade 70 is generally not acceptable for severe sour environments.
Is A516 Grade 70 killed steel?
Yes, ASTM A516 Grade 70 is a fully killed carbon steel.
Can A516 Grade 70 be used for cryogenic service?
Yes, ASTM A516 Grade 70 can be used for mild low-temperature and light cryogenic service down to -46°C (-50°F), but it is not suitable for deep cryogenic applications (such as liquid nitrogen or liquid helium).
Is impact testing mandatory for A516 Grade 70?
No, impact testing is not automatically mandatory for standard ASTM A516 Grade 70 steel plate.