S355J2 is one of the most widely used structural steel plate grades in the world. It belongs to the non-alloy structural steel family covered by EN 10025-2, the European standard for hot-rolled products of structural steels. The designation splits into three parts. The number 355 is the minimum yield strength in MPa for the thinner end of the thickness range. The letter J indicates that the steel is impact tested with a Charpy V-notch specimen, and the number 2 fixes the impact test temperature at -20 C, with a minimum absorbed energy of 27 J. In practice S355J2 delivers a 355 MPa strength class together with reliable notch toughness below freezing, which is why it dominates bridge, building and heavy machinery work in Europe and is widely ordered elsewhere as an equivalent to local grades.
Chemical Composition
EN 10025-2 keeps the chemistry deliberately lean, because a low carbon equivalent is what makes a structural steel easy to weld and to form. The limits below are typical of the ladle analysis specified for S355J2 plate.
| Element | Limit (%) |
|---|---|
| C | 0.20 max (lower for heavy thicknesses as agreed at ordering) |
| Si | 0.55 max |
| Mn | 1.60 max |
| P | 0.025 max |
| S | 0.025 max |
| Cu | 0.55 max |
| N | 0.012 max |
Sulphur and phosphorus are capped because both damage toughness and weldability, and nitrogen is limited to prevent strain ageing in the heat-affected zone. The grade is fully killed and fine grain treated, normally with aluminium, so that the impact requirement at -20 C can be met consistently.
Mechanical Properties and Impact Requirements
The guaranteed properties of S355J2 depend on plate thickness. Minimum yield strength steps down as the section becomes heavier, while the tensile range and the impact class remain unchanged.
| Thickness (mm) | Yield strength, min (MPa) | Tensile strength (MPa) | Elongation, min (%) |
|---|---|---|---|
| Up to 16 | 355 | 470 - 630 | 22 |
| Over 16 to 40 | 345 | 470 - 630 | 22 |
| Over 40 to 63 | 335 | 470 - 630 | 21 |
| Impact class | Charpy V-notch, 27 J minimum at -20 C | ||
Delivery Conditions and Related Grades
S355J2 plate is commonly supplied in the normalized condition, and the normalized route is the safest choice when the plate will be hot formed or when toughness must be verified after fabrication. Two related options are worth knowing. S355J2 is also produced in the as-rolled condition in some thickness ranges, but the higher carbon content that this allows reduces toughness and weldability, so it is specified only where the application permits. Where a lower carbon equivalent is needed for heavy welding, thermomechanically rolled grades such as those covered by EN 10025-4 offer the same strength class with better welding behaviour, at the cost of tighter limits on hot forming and post-weld heat treatment.
Forming, Cutting and Welding of S355J2
Cutting: shearing, plasma and oxy-fuel cutting all work normally. Flame-cut edges on thick restrained plate benefit from removal of the hardened layer before welding or service.
Cold forming: the grade has ample ductility for rolling, pressing and bending. Minimum bend radii follow the thickness and the rolling direction, and tight radii in heavy plate should be checked against the applicable fabrication standard.
Welding: S355J2 welds readily with all common arc processes. Consumables are matched to the tensile class, hydrogen-controlled consumables are used for thick or restrained joints, and preheat is applied as a function of thickness, carbon equivalent and restraint. The carbon equivalent is typically around 0.45 % maximum, which keeps preheat requirements moderate rather than severe.
Post-weld heat treatment: stress relief is applied where required by the design code, with the soaking temperature kept below the lower transformation temperature to avoid loss of strength and toughness.
Applications and National Equivalents
S355J2 is used for bridge girders and deck plates, building frames and columns, transmission and communication towers, crane and lifting equipment, power station structures, storage tanks, transport equipment and general welded fabrications that carry heavy loads. Its combination of strength, toughness and weldability also makes it a common choice for cold-formed sections and for machined components where a low-alloy high-strength structural steel is adequate without the cost of an alloy grade. In China the matching grade is Q355D of GB/T 1591, which replaced the older Q345D designation when the standard was revised, and both require impact testing at -20 C. Other systems have analogous grades, such as S355J2 in European practice against similar normalized 355 MPa classes elsewhere, and the correct comparison is always made on the basis of chemistry limits, impact temperature and thickness-dependent property tables rather than on a simple name match.
Frequently Asked Questions
Q: What does J2 mean in S355J2?
J2 identifies the impact class: Charpy V-notch specimens must absorb at least 27 J at a test temperature of -20 C. A plain S355JR grade is tested at room temperature only, and S355J0 is tested at 0 C.
Q: Is S355J2 equivalent to Q355D?
Yes, Q355D of GB/T 1591 is the nearest Chinese equivalent, with the same 355 MPa yield class and impact testing at -20 C. The older Q345D grade has been superseded by Q355D in the current standard.
Q: Which standard governs S355J2?
EN 10025-2 covers hot-rolled non-alloy structural steels and contains the S355J2 requirement, including chemistry limits, thickness-dependent mechanical values and the -20 C impact class.
Q: Can S355J2 be welded without preheat?
For thin plate and light restraint, welding is often possible without preheat, but thickness, carbon equivalent, restraint and hydrogen level must be assessed together. Thick or highly restrained joints normally call for controlled preheat and interpass temperature.
Q: Is S355J2 suitable for low-temperature service?
It is qualified for impact testing at -20 C, so it suits many cold-climate structures. Below that temperature a design assessment is required, and steels with lower transition temperatures are usually selected.
Q: How does S355J2 differ from S355JR?
Both share the same strength requirements, but S355JR is impact tested at room temperature while S355J2 is tested at -20 C. The J2 grade therefore requires finer grain control and tighter chemistry, which makes it the safer choice for structural work in cold environments.