12Cr1MoVR Pressure Vessel Steel Plate: Composition, Properties and GB/T 713 Data

What 12Cr1MoVR Pressure Vessel Steel Plate Is

12Cr1MoVR is a chromium-molybdenum low-alloy steel plate developed for high-temperature and high-pressure service. It belongs to the family of Cr-Mo vessel steels and is produced to the Chinese pressure vessel plate standard GB/T 713, where the 2023 revision splits the former GB 713-2014 into a series of parts and carries this grade in the Cr-Mo part. The final letter "R" identifies the product as a vessel plate, while "12" denotes a nominal carbon content of 0.12 %, "Cr" chromium, "Mo" molybdenum and "V" vanadium.

The steel is designed on the low-alloy high-strength concept: a balanced alloy addition combined with controlled heating and cooling produces a fine microstructure that delivers useful strength with adequate ductility and toughness. Compared with plain carbon vessel steels, 12Cr1MoVR offers markedly better oxidation resistance and creep-rupture strength in the elevated-temperature range for which it is qualified, which is why it is widely specified for petrochemical reactors, regenerators, furnace tubes and nuclear power plant pressure components.

Chemical Composition of 12Cr1MoVR

The table below lists the heat analysis limits normally applied to 12Cr1MoVR plate. Chromium and molybdenum provide solid-solution strengthening and carbide stability at temperature, vanadium refines the carbide distribution and improves creep resistance, while phosphorus and sulphur are held at low levels to protect toughness and weldability.

Element C Si Mn Cr Mo V Cu Ni P S
12Cr1MoVR, % 0.08-0.15 0.15-0.40 0.40-0.70 0.90-1.20 0.25-0.35 0.15-0.30 ≤0.30 ≤0.30 ≤0.025 ≤0.010

Carbon is kept in the medium-low range so that strength is obtained mainly through alloy carbides rather than through a high carbon content, which would harm toughness and welding behaviour. The chromium level of roughly one percent is the key to the grade's oxidation resistance; molybdenum and vanadium together control the coarsening of carbides during long exposure at temperature.

Mechanical Properties

Tensile and yield requirements are specified against plate thickness because the through-thickness microstructure of a quenched-and-tempered or normalised plate varies with section size. Room-temperature values for 12Cr1MoVR are summarised below.

Steel grade Thickness, mm Tensile strength, MPa Yield strength, min, MPa Elongation, min, %
12Cr1MoVR 6 < T ≤ 60 440-590 245 19
12Cr1MoVR 60 < T ≤ 100 430-580 235 19

Thicker plate is tested on the same principle but with the reduced strength range shown, reflecting the slower cooling rate at mid-thickness. Charpy V-notch impact testing is performed on the standard test temperature defined for the grade, and the result is reported together with the tensile data on the mill certificate so that the plate can be released for pressure equipment fabrication.

Heat Treatment and Delivery Condition

12Cr1MoVR is normally supplied in the normalised and tempered condition, which produces a uniform ferrite-bainite microstructure and the best combination of strength, ductility and impact toughness. On special agreement at the ordering stage the plate can also be delivered in the annealed or tempered condition, for example when a customer's forming route requires a softer starting structure. Because the grade depends on a controlled heating and cooling cycle to develop its properties, the delivery condition must always be stated in the purchase order and confirmed on the inspection certificate.

Thickness tolerances follow GB/T 709, which replaced the earlier GB 709 edition; the Class B deviation is the usual minimum requirement for vessel plate, and tighter limits can be negotiated for plate that will be cold formed.

Fabrication: Welding, Forming and Post-Weld Heat Treatment

The grade is readily welded by shielded metal arc, submerged arc and gas tungsten arc processes using matching Cr-Mo filler metals. Because of its alloy content and hardenability, a moderate preheat is normally applied before welding, especially on thick sections, and interpass temperature is controlled to avoid excessive grain growth. Post-weld heat treatment is standard practice for pressure components in this grade: it relieves residual stress, tempers the heat-affected zone and restores toughness. Fabricators should design the heat treatment cycle to stay within the temperature and time window agreed for the grade, since over-tempering reduces strength while under-tempering leaves a hard, brittle zone.

Cold forming of normalised and tempered plate is practical up to moderate strain levels; heavier cold deformation or flame straightening should be followed by a stress-relief treatment. Hot forming is carried out in a controlled temperature range followed by a fresh normalising and tempering cycle so that the specified properties are re-established.

Applications and Grade Selection

Petrochemical equipment: hydrotreating and hydrocracking reactors, regenerators, heat exchangers and furnace tubes.

Power and nuclear plant: high-pressure vessel shells, headers and steam-side components.

General high-temperature pressure equipment: coke drums, gasification vessels and ammonia synthesis housings.

Where service temperature or hydrogen partial pressure rises beyond the capability of 12Cr1MoVR, designers step up to higher-chromium grades such as 12Cr2Mo1R, which carries more chromium and molybdenum for improved creep strength and hydrogen resistance. Where the duty is cooler and less demanding, a carbon-manganese vessel plate such as 15CrMoR or a plain Q245R plate is usually more economical. Selecting the correct grade therefore depends on design temperature, design pressure, hydrogen exposure and the corrosion allowance required by the governing design code.

Frequently Asked Questions

Q: What does the designation 12Cr1MoVR mean?
The number 12 indicates a nominal carbon content of about 0.12 %, Cr, Mo and V indicate chromium, molybdenum and vanadium additions, and R marks the steel as a vessel plate in the Chinese GB system.

Q: Which standard covers 12Cr1MoVR steel plate?
It is specified in the GB/T 713 pressure vessel steel plate standard series, which replaced GB 713-2014; thickness tolerances are normally taken from GB/T 709 Class B.

Q: In what condition is the plate delivered?
The standard delivery condition is normalised and tempered. Annealed or tempered delivery can be arranged by special agreement when the fabrication route requires it.

Q: Why is post-weld heat treatment required?
Welding creates residual stress and a hardened heat-affected zone; a controlled post-weld heat treatment relieves stress, tempers that zone and restores impact toughness in Cr-Mo pressure components.

Q: How does 12Cr1MoVR compare with 12Cr2Mo1R?
12Cr2Mo1R contains roughly twice the chromium plus higher molybdenum, giving better creep strength and hydrogen resistance; it is chosen for more severe high-temperature or hydrogen-charged service.

Q: Is the steel suitable for low-temperature applications?
It is intended for elevated-temperature pressure service. For low-temperature duties, grades with higher nickel content or a dedicated low-temperature impact designation should be selected instead.