Mar 08, 2024 Leave a message

SNCM220 Chromium-Molybdenum Case Hardening Steel: JIS G4053 Composition and Heat Treatment

SNCM220 is a chromium-molybdenum low alloy steel for machine structural use, standardised in JIS G4053 and widely produced in round bar and wire rod. It is a case-hardening grade: the core stays tough and shock resistant while the carburized surface is hardened to resist wear. That combination is the reason the grade dominates small and medium sized transmission parts such as gears, shafts, pins and bearing components that run under repeated loading.

Chemical Composition to JIS G4053

Nickel improves core toughness and hardenability without raising the carbon level, chromium supplies wear resistance and response to heat treatment, and molybdenum suppresses temper embrittlement and stabilises the case. Limits below are ladle analysis in mass percent.

Element C Si Mn P S Ni Cr Mo Cu
SNCM220 0.17-0.23 0.15-0.35 0.60-0.90 max 0.030 max 0.030 0.40-0.70 0.40-0.60 0.15-0.30 max 0.30

Equivalent designations used when converting drawings between systems include the 8620 family in the SAE and AISI scheme, 20NiCrMo2-2 in EN 10084 for case-hardening steels, and 20CrNiMo in GB/T 5216. The chemical ranges overlap closely, but hardenability bands and residual element limits are not identical, so substitution should be confirmed against the governing drawing and heat treatment specification rather than by name alone.

Heat Treatment Practice

The grade responds predictably to a conventional carburize, direct quench and temper route. Typical shop practice is to carburize in the range 900 to 930 degrees C, control the case depth by holding time at temperature, quench in oil from about 830 to 860 degrees C, and temper between 150 and 200 degrees C to relieve stress while keeping case hardness. Normalizing before machining refines the structure of bar stock and improves dimensional stability during later hardening.

Step Typical temperature (C) Purpose
Normalizing 870-900 Refine grain, homogenise structure before machining
Carburizing 900-930 Carbon-rich case, depth set by holding time
Direct quench 830-860, oil Harden case, retain soft core
Tempering 150-200 Relieve stress, stabilise case hardness

Case, Core and Property Balance

Case depths commonly specified for this grade are 0.5 mm to 1.5 mm. After correct treatment the surface normally reaches roughly 58 to 62 HRC on a Rockwell C scale while the core remains in the region of 30 to 42 HRC, which gives the part a hard, wear resistant skin over a matrix that can absorb impact without cracking. Where higher core strength is needed, the design usually moves to a leaner case depth combined with a lower tempering temperature, or to a different grade with a higher hardenability, rather than by over-carburizing SNCM220.

Machinability, Formability and Inspection

Supplied in the annealed or normalized condition, the steel machines well with coated carbide tooling and is readily hobbing, broaching and thread-cutting friendly for mass production. Finish machining is normally carried out before hardening, with grinding allowance left for the case-hardened surfaces. Dimensional control after treatment matters because quenching distortion in thin-walled parts can exceed the tolerance band; for critical gears, distortion is managed by fixture quenching and by leaving stock for hard finishing. Hardness surveys, case depth measurement on a sectioned witness sample, and magnetic particle inspection for surface cracks are the standard verification steps.

Typical Applications

Automotive transmission shafts, drive shafts, crankshaft sprockets and differential gears; pins, bushes and cam followers in general machinery; gearbox internals in mining and construction equipment that see shock loading as well as abrasion; and engine accessory shafts. The grade is chosen wherever a hard running surface has to coexist with a core that will not shatter under overload.

Frequently Asked Questions

Q: Is SNCM220 the same as 8620?
A: They are close equivalents that are frequently interchanged, but the specified limits differ. SNCM220 is defined in JIS G4053 while 8620 sits in the SAE and AISI system, so the controlling drawing should be checked before substitution is approved.

Q: What is the hardness after carburizing SNCM220?
A: Typical practice gives roughly 58 to 62 HRC at the case surface with a core around 30 to 42 HRC, depending on case depth and tempering temperature.

Q: How deep should the carburized case be?
A: For most gears and shafts the working range is 0.5 mm to 1.5 mm effective case depth, selected from the contact stress and the permissible core load rather than from a fixed rule.

Q: Can SNCM220 be welded?
A: It can be welded with preheat and controlled cooling, but the grade is designed for case hardening rather than for welded fabrication, and welded joints in hardened parts are normally avoided on principle.

Q: Why is chromium and molybdenum present?
A: Chromium raises hardenability and wear resistance in the case, while molybdenum improves hardenability of the core, resists temper embrittlement and keeps the case from softening during carburizing.

Q: What form is SNCM220 supplied in?
A: Round bar and wire rod in the annealed, normalized or as-rolled condition, in diameters suited to machining or cold forming, with bar end hardening tests used to confirm hardenability where it matters.