Mar 26, 2024 Leave a message

SPV235 Pressure Vessel Steel Plate: JIS G 3115 Grades and Welding

SPV235 Within the JIS G 3115 Framework

SPV235 is the lowest-strength grade in the JIS G 3115 series, the Japanese standard for steel plates used in pressure vessels serving at intermediate temperature. The grade designation is read in two parts: SPV marks a steel plate for pressure vessels, and 235 states the minimum specified yield strength in newtons per square millimetre. In trade correspondence the material is often described as a container plate, a literal translation of the vessel-plate usage, but the technical identity of the product is defined entirely by JIS G 3115 and by the mill certificate issued against it.

The distinction between JIS G 3115 and JIS G 3103 matters at the ordering stage. JIS G 3103 covers boiler and pressure vessel plates for moderate and ordinary service temperatures, where SB410 and SB450 are the familiar designations. JIS G 3115 exists for vessels that must retain notch toughness at temperatures below ambient, which is why every grade in the series carries a mandatory Charpy V-notch impact test as part of the delivery requirement rather than as an optional supplement. A purchaser who accepts an SB410 plate in place of an SPV235 plate receives a material of similar tensile level but without the same guaranteed toughness regime.

Plate thickness for the SPV series conventionally runs from 6 mm up to 200 mm, although the practical availability of any single grade narrows at the heavy end and at the light end. SPV235 is most often rolled between 8 mm and 60 mm, which covers the shell courses, heads and nozzle reinforcement of shop-fabricated vessels, air receivers, separators and storage bullets. Above roughly 80 mm the tonnage demand per heat rises sharply and mill rolling schedules become the limiting factor rather than the grade itself.

Grade Ladder: Where SPV235 Sits

The SPV series is a strength ladder, not a set of interchangeable materials. Each step adds tensile capability at the cost of toughness margin and weldability, because the alloy addition and the carbon equivalent that raise strength also raise hardenability in the heat-affected zone. Reading the ladder as a whole is the fastest way to decide whether SPV235 is sufficient for a given design pressure and shell thickness.

Grade Minimum yield strength, MPa Tensile strength range, MPa Typical service role
SPV235 235 400 - 510 Low-pressure vessels, receivers, storage bullets, penstocks
SPV315 315 490 - 610 Medium-pressure shells, heat exchanger bodies
SPV355 355 520 - 640 Thicker shells where weight reduction is required
SPV410 410 550 - 690 High-pressure separators, heavy-wall reactors
SPV490 490 610 - 740 Very high pressure and large diameter spheres

Minimum elongation is graded by thickness inside the standard and falls as the strength level rises, from roughly 25 percent for thin SPV235 plate to about 17 percent for the high-strength end of the series. A designer who substitutes a higher grade to save thickness must re-check nozzle reinforcement, weld procedure qualification and post-weld heat treatment, because a thinner high-strength shell changes both the restraint pattern and the cooling rate of every weld made on it.

Chemical Composition and Clean Steel Practice

JIS G 3115 frames the chemistry of SPV235 around a low-carbon, manganese-killed analysis with deliberate limits on phosphorus and sulphur. The values below are representative production ranges seen on mill certificates for the grade; they describe normal good practice and are not a substitute for the composition limits printed in the standard or agreed on the purchase order.

Element Typical range, % Purchasing significance
Carbon 0.14 - 0.19 Controls tensile level and HAZ hardness; keeps carbon equivalent low
Silicon 0.15 - 0.35 Deoxidation; excess raises slag fluidity problems in welding
Manganese 0.70 - 1.20 Strength and toughness balance; part of the carbon equivalent
Phosphorus 0.020 max Temper embrittlement and thickness-direction ductility
Sulphur 0.010 max Drives inclusion shape and lamellar tearing risk
Aluminium, total 0.020 min Fine grain practice; essential for the impact guarantee

Two chemical decisions decide whether an SPV235 plate behaves well in fabrication. The first is fine grain practice through aluminium addition or an equivalent nitride-forming treatment, without which the Charpy requirement at the specified test temperature becomes difficult to hold consistently at heavy gauge. The second is sulphur control combined with calcium treatment for plates that will be welded under high restraint. Calcium modifies elongated manganese sulphide into globular inclusions that do not open up as planes parallel to the rolling surface, which is precisely the failure mode that through-thickness testing is designed to expose.

Carbon equivalent is not the only number worth requesting. For plate intended for cold forming of heads, a carbon equivalent calculated on the basis of the actual heat analysis, together with the reported aluminium and nitrogen, gives a far better prediction of forming behaviour than the tensile result alone. Where the vessel will be stress relieved after welding, the reported residual element levels, particularly copper, tin and antimony, influence how much toughness is lost during the heat treatment.

Mechanical Property Verification

Tensile testing follows the Japanese tensile test standard JIS Z 2241, with the test piece orientation and location defined so that results are comparable between mills. The specified yield strength of 235 MPa is a minimum, not a target: production heats for the grade commonly test between 260 MPa and 320 MPa, and a plate that tests far above the minimum usually signals a carbon or manganese content at the top of the range, which in turn predicts higher hardness in the heat-affected zone.

Sampling practice deserves scrutiny on thick plate. Test pieces are taken from a location that represents the mid-width of the plate, and for heavy gauge the through-thickness position of the test coupon determines how representative the result is of the material at the quarter-thickness level, where the vessel shell actually carries stress. Purchasers of plate above 40 mm should confirm on the certificate that the tensile and impact coupons were taken after the final heat treatment, since a plate normalised after sampling would otherwise be certified on properties that no longer describe the delivered product.

Retest rules are part of the acceptance conversation. When a single tensile or impact result falls outside the requirement, the standard permits retesting on additional coupons from the same lot under defined conditions, and the number of retests permitted is limited. A certificate that shows several successive retests on the same heat is a warning sign about process stability rather than a routine administrative detail.

Charpy Impact Testing and the Intermediate Temperature Requirement

The impact test is the feature that separates JIS G 3115 material from ordinary structural plate. Charpy V-notch testing is performed to JIS Z 2242 on full-size 10 mm by 10 mm specimens where the plate thickness allows, and the ordinary acceptance rule is an average absorbed energy of 47 J across three specimens with no individual value below 70 percent of that average. When the plate is too thin for a full-size specimen, sub-size specimens are used and the acceptance energy is scaled accordingly, so a certificate for 8 mm plate should be read against the sub-size requirement rather than the full-size figure.

Test temperature is fixed by the grade and by the order. Because SPV235 addresses intermediate temperature service, the standard test temperature sits close to ambient, and projects that need verification at a lower temperature place a supplementary requirement on the order. That supplement is not cosmetic: the ductile-to-brittle transition of a 235 MPa ferritic plate is broad, and the energy absorbed at minus 20 degrees Celsius can be a small fraction of the value measured at zero. Vessels that will be hydrotested with cold water, installed in unheated structures, or purged with cold gas should carry the low-temperature supplement explicitly in the purchase specification.

Specimen axis orientation also changes the number. Transverse specimens, taken across the rolling direction, normally give lower absorbed energy than longitudinal specimens. Mixing the two orientations across a delivery makes two plates of the same heat appear to have different toughness, so the orientation should be stated once and applied to every test in the lot.

Thickness, Tolerances and Mass Calculation

Dimensions and permissible variations for hot rolled plate are governed by JIS G 3193. The tolerance band on thickness is asymmetric in practice, with a smaller minus allowance than plus allowance, because a plate rolled slightly heavy is acceptable to a fabricator whereas a plate rolled under nominal thickness erodes the corrosion allowance and, in some designs, the pressure rating. For a vessel with a 3 mm corrosion allowance on a 12 mm shell, a plate at the bottom of the minus tolerance removes a measurable part of the design margin before the vessel ever enters service.

Mass is calculated from nominal dimensions using a density of 7.85 tonnes per cubic metre for carbon and low-alloy steel: mass in kilograms equals thickness in millimetres multiplied by width in metres, multiplied by length in metres, multiplied by 7.85. Theoretical mass and actual weighed mass diverge when the plate sits at the top of the thickness tolerance, which is why export contracts should state whether invoicing follows theoretical or actual weight. The difference on a 40 mm plate at the plus tolerance is commonly between one and two percent of invoice value across a full order.

Flatness, camber and squareness are separate acceptance items from thickness. Plate for shell rolling must be flat enough to enter the rolls without buckling, and plate for head pressing must be free of pronounced crown. Specifying flatness by reference to JIS G 3193, and stating the fabrication step the plate is destined for, prevents a delivery that meets the thickness clause but cannot be rolled without re-flattening.

Through-Thickness Quality: Z15, Z25 and Z35

Z-direction quality addresses lamellar tearing, the step-like fracture that opens parallel to the plate surface when a weld shrinks against the through-thickness direction of a thick plate. The mechanism is inclusion-driven, so the qualifying test is a tensile test loaded through the plate thickness, and the acceptance criterion is the reduction of area at fracture. Through-thickness characteristics for pressure vessel plate are specified in JIS G 3199, with Z15, Z25 and Z35 denoting minimum reduction of area of 15, 25 and 35 percent respectively.

Designation Minimum reduction of area, % Where it is normally specified
Z15 15 Moderate restraint, nozzle welds in medium thickness
Z25 25 Heavy nozzle reinforcement, box girders, corner joints
Z35 35 Severe restraint, thick-section T and corner joints, lifting points

Ordering Z quality changes the steelmaking route rather than the rolling route. Sulphur is driven well below the level used for ordinary plate, inclusion shape is controlled, and the plate is normally subjected to ultrasonic inspection to demonstrate freedom from internal discontinuities. The practical consequence for a fabricator is a shorter and more expensive supply chain, so Z quality should be applied to the specific plates that carry through-thickness stress rather than to an entire vessel.

Reduction of area is verified on specimens taken in the through-thickness direction, which requires a plate thick enough to machine a suitable coupon. Z quality is therefore rarely meaningful below about 16 mm and is usually ordered in the 20 mm to 150 mm range, where the geometry of the joint actually generates through-thickness strain.

Ultrasonic Testing Classes

Internal soundness is verified by ultrasonic testing to JIS G 0901, which defines several testing classes of increasing severity. The class chosen determines the probe arrangement, the scanning grid and the size of discontinuity that must be recorded, and the corresponding acceptance criteria define whether a recorded indication rejects the plate, requires repair by grinding within the thickness allowance, or is acceptable as reported.

A practical ordering rule is to match the UT class to the consequence of failure. Plates for a low-pressure receiver on a skid may be accepted against a routine class; plates for a thick reactor shell, a sphere or a vessel in cyclic service should be specified at a higher class, with the reflected indications mapped so that nozzle locations can be positioned away from any recorded area. When Z quality is ordered, UT is effectively inseparable from it, because the reduction-of-area test proves the average cleanliness of a coupon while UT proves the local condition of the actual plate.

Delivery Condition and Heat Treatment

SPV235 is supplied in the as-rolled, normalised or normalised-rolled condition, and the condition stated on the certificate must match the condition of the plate delivered. Normalising consists of austenitising the plate, holding at temperature long enough to homogenise the structure, and cooling in still air; the result is a fine, uniform ferrite-pearlite structure with predictable and reproducible impact behaviour. Normalised rolling achieves a similar result by finishing the rolling pass sequence within a controlled temperature window, avoiding a separate furnace cycle.

For the 235 MPa grade, normalising temperatures sit in the region of 900 degrees Celsius, with the soak determined by thickness rather than by grade. Two points matter to the purchaser. First, plate that has been subjected to a shop normalising cycle after delivery must be re-certified or at least re-tested, because the mechanical properties certified at the mill no longer describe the plate. Second, repeated normalising is not a neutral operation: each cycle coarsens the grain if the temperature is allowed to run high, and the toughness lost that way is not recoverable by a subsequent temper.

Quenching and tempering is not the standard route for SPV235 and should not be accepted as an equivalent without a documented procedure qualification, since the higher strength obtained by quenching changes both the design basis and the welding consumable selection.

Welding and Fabrication Practice

SPV235 welds with the consumables used for the 400 MPa tensile class of carbon-manganese steels. Shielded metal arc, gas metal arc and submerged arc processes are all routine, and the governing variables are heat input, interpass temperature and the cleanliness of the joint preparation. Because the carbon equivalent of the grade is low, preheat is usually unnecessary below about 25 mm for restrained joints in temperate conditions, but preheat of 100 to 150 degrees Celsius becomes prudent for thicker sections, for high restraint joints, and for fabrication in a cold shop where the plate surface sits near freezing.

Hydrogen control is the underlying reason rather than temperature for its own sake. Low-hydrogen consumables, baked electrodes and clean, dry joint faces reduce the diffusible hydrogen that causes delayed cracking under restraint. Where a Z-quality plate is welded into a corner joint, the through-thickness strain concentrates at the fusion boundary, and a weld that would be sound in a butt joint can open a lamellar tear in a T joint at the same heat input.

Post-weld heat treatment for stress relief is typically carried out in the 580 to 620 degrees Celsius range with a controlled heating and cooling rate scaled to thickness, holding one hour per 25 mm of section with a minimum hold. The treatment relieves residual stress and softens the hardened zone, but it also tempers the plate itself, so the procedure qualification should demonstrate that both weld and parent metal still satisfy the specified tensile and impact requirements after the cycle.

Applications and Grade Selection

SPV235 plate is used for liquefied petroleum gas storage bullets, air receivers, compressed gas receivers, oil and water separators, heat exchanger shells at moderate pressure, penstock linings and the casings of hydroelectric equipment. These applications share a design pressure that a 235 MPa yield material can carry at economic wall thickness, and a service temperature that does not demand elevated-temperature creep data or low-temperature toughness beyond the supplementary requirement.

Moving up the ladder should be a design decision, not a procurement convenience. If the calculated shell thickness at SPV235 exceeds roughly 40 mm for a vessel in cyclic service, the weld restraint, the post-weld heat treatment burden and the inspection cost usually justify evaluating SPV315 or SPV355 instead, even though the material cost per tonne is higher. Conversely, specifying SPV355 for a small receiver that a 10 mm SPV235 shell would satisfy adds cost and reduces toughness margin for no engineering benefit.

Inspection, Documentation and Common Mistakes

A complete delivery package for SPV235 plate includes the mill test certificate to EN 10204 type 3.1, showing heat number, product analysis, tensile and impact results with test temperatures, the delivery condition, and the UT class where specified. The heat number on the certificate must be traceable to the stencil or stamp on the plate, and the plate marking should survive fabrication handling long enough to be transferred to the cut parts.

Three errors recur in procurement of this grade. The first is accepting boiler plate to JIS G 3103 as an equivalent, which overlooks the different impact regime. The second is treating an as-rolled plate as normalised because the tensile result was satisfactory; tensile strength does not demonstrate toughness uniformity. The third is ordering UT and Z quality verbally and finding neither on the certificate, which usually becomes visible only when a third-party inspector arrives at the fabricator's shop.

Storage, Handling and Safety

Plate should be stored clear of the ground on timber or steel bearers spaced to prevent sag, with the stack arranged so that water drains rather than pools between plate surfaces. Edge protection matters for plate destined for shell rolling, since a lifted plate with a deformed edge will produce an oval course. Lifting should use plate clamps or slings rated for the load, never the lifting holes burned by the fabricator without an engineering check.

Cutting and welding generate fume and ultraviolet radiation, so local extraction and appropriate eye and skin protection are required at every station. Grinding dust from plate that has been shop-primed should be treated as a coating hazard rather than as steel dust, particularly where zinc-rich primers are involved.

FAQ

Q: What does the 235 in SPV235 actually guarantee?
It guarantees a minimum yield strength of 235 MPa together with a tensile strength between 400 and 510 MPa, and it is the strength floor of the JIS G 3115 ladder rather than a target value. Production heats commonly test well above the minimum.

Q: Is SPV235 the same as SB410 from JIS G 3103?
The tensile ranges overlap closely, but the two belong to different standards with different toughness requirements. JIS G 3115 couples the grade to a mandatory Charpy V-notch test, so SB410 should not be substituted without a documented design review.

Q: When should Z15, Z25 or Z35 be added to the order?
When the joint geometry loads the plate through its thickness, typically at thick nozzle reinforcement, corner joints and lifting attachments, and when restraint during welding is high. The requirement is defined in JIS G 3199 by minimum reduction of area in the through-thickness direction.

Q: Does SPV235 need preheat before welding?
For thin plate in moderate ambient conditions, normal good practice with low-hydrogen consumables is usually sufficient. Preheat of 100 to 150 degrees Celsius becomes advisable above roughly 25 mm, for high restraint joints, and for cold workshop conditions.

Q: How is the weight of an SPV235 plate calculated?
From nominal dimensions using a density of 7.85 tonnes per cubic metre: thickness in millimetres times width in metres times length in metres times 7.85 gives the mass in kilograms. Theoretical and weighed mass diverge when plate sits at the top of the thickness tolerance.

Q: Can a normalised plate be normalised again at the fabricator's shop?
It can, but the plate must then be re-tested, because the certified properties apply to the condition as delivered. Repeated cycles at excessive temperature coarsen the grain and reduce impact energy in a way that cannot be recovered afterwards.

Send Inquiry

whatsapp

phone

Email

Inquiry