Jan 08, 2026 Leave a message

ASTM A387 Grade 11 Class 2 Steel Plate: Properties and Uses

What Is ASTM A387 Grade 11 Class 2 Steel?

ASTM A387 Grade 11 Class 2 is a chromium-molybdenum alloy steel plate specified for weldable pressure vessels, boilers and heat exchangers that operate at elevated temperature. The grade carries a nominal composition of about 1.25% chromium and 0.50% molybdenum. Class 2 denotes the higher-strength delivery condition: the plate is normalized and tempered, which raises the mechanical properties well above the Class 1 level while retaining weldability and toughness. Under the ASME Boiler and Pressure Vessel Code the same material is designated SA387 Grade 11 Class 2, with identical chemistry and mechanical requirements.

Chemical Composition

The heat-analysis limits for A387 Grade 11 are:

Element C Mn Si P S Cr Mo
Range / max (%) 0.05–0.17 0.40–0.65 0.50–0.80 0.035 max 0.035 max 1.00–1.50 0.45–0.65

Chromium provides oxidation and corrosion resistance at high temperature; molybdenum adds creep strength; and the silicon range supports deoxidation during steelmaking. The restricted phosphorus and sulfur limits protect toughness and weldability in thick plate.

Mechanical Properties: Class 2 vs Class 1

Minimum room-temperature values for Grade 11 plates:

Property Class 2 (N&T) Class 1
Tensile strength (ksi / MPa) 75–100 / 515–690 60–85 / 415–585
Yield strength, min (ksi / MPa) 45 / 310 30 / 205
Elongation in 8 in, min 18% 18%
Elongation in 2 in, min 22% 22%

Because Class 2 is normalized and tempered, it carries higher design stress at elevated temperature, which translates into thinner vessel walls and lower fabrication cost for the same duty.

Commonly Cited Equivalents

The most frequently cited equivalents for A387 Grade 11 are ASME SA387 Grade 11 (the same material under ASME rules) and EN 10028-2 13CrMoSi5-5 (material number 1.7335) in European practice, along with the historical UK designation BS 1501-621. Equivalence should be verified against both specifications for the project, since composition tolerances and delivery conditions differ in detail.

Typical Applications

Grade 11 Class 2 plates are used for pressure vessels, boiler drums, heat exchangers and related equipment in oil and gas processing, petrochemical plants and power generation. The material is selected where service temperatures are high enough that ordinary carbon-manganese steels lose allowable stress, but where the full high-temperature capability of a 2.25Cr–1Mo grade such as Grade 22 is not required. Its good weldability with low-hydrogen processes and its resistance to oxidation make it a workhorse alloy plate in elevated-temperature fabrication.

Frequently Asked Questions

What is the difference between Class 1 and Class 2?

Class 2 is supplied normalized and tempered, with a minimum yield strength of 310 MPa (45 ksi) and tensile strength of 515–690 MPa; Class 1 has 205 MPa (30 ksi) minimum yield and 415–585 MPa tensile. The higher-strength Class 2 allows thinner vessel walls.

Is A387 Grade 11 equivalent to 13CrMoSi5-5?

EN 10028-2 13CrMoSi5-5 (1.7335) is the closest commonly cited European equivalent for A387/SA387 Grade 11. Composition and strength are close, but delivery condition and acceptance criteria should be checked against both standards.

Does Grade 11 Class 2 require impact testing?

Charpy impact testing is not mandatory by default in ASTM A387. It is added as a supplementary or project requirement with an agreed test temperature and energy, typically verified against the mill test certificate.

What is the difference between Grade 11 and Grade 22?

Grade 11 is 1.25% Cr–0.5% Mo; Grade 22 is 2.25% Cr–1.0% Mo. Grade 22 offers higher creep strength and oxidation resistance for more severe elevated-temperature and hydrogen service, at a higher cost.

Can Grade 11 Class 2 be welded?

Yes, with low-hydrogen processes and consumables matching the 1.25Cr–0.5Mo chemistry. Preheat and post-weld heat treatment requirements follow the governing code and plate thickness.

Where is A387 Grade 11 Class 2 typically used?

Typical uses include pressure vessels, boilers, heat exchangers and piping-related components in oil and gas, petrochemical and power generation facilities operating at elevated temperature.