What "Raw Material" Means in a Stainless Medium Plate Mill
The phrase raw material hides three different inputs in a stainless steel medium plate plant, and buyers who do not separate them end up comparing offers that are not comparable. The first input is the metallic charge that becomes one heat of steel: stainless scrap, carbon steel scrap, ferroalloys and pure metals weighed into a furnace. The second is the semi-finished product that leaves the caster or the ingot yard: a slab, a bloom or a transfer bar. The third, in re-rolling and cut-to-length operations, is a coil: either a hot rolled annealed and pickled coil that is decoiled, levelled and cross-cut into plate, or a cold rolled hard coil that is slit and cut for a different family of products.
For a 3 mm to 20 mm medium plate the usual chain is electric arc furnace melting, argon oxygen decarburization, continuous casting into a slab of roughly 180 mm to 220 mm thickness, reheating, roughing, finishing in a hot strip or plate mill, then annealing and pickling to the No.1 finish. For heavy plate above 40 mm, or for grades that cannot tolerate the cooling rate of a caster, the chain starts from an ingot or an electroslag remelted slab instead. Knowing which chain a mill intends to use is the single most useful question a plate buyer can ask, because the answer determines the achievable thickness tolerance, the flatness, the soundness of the centre line and the surface finish that can be quoted at a given price.
The Metallic Charge: Scrap, Ferroalloys and Residual Control
A stainless heat is not made from ore in an integrated steelworks sense; it is made from carefully classified scrap plus alloy carriers. The charge design fixes the nickel, chromium and molybdenum balance before any refining step, and refining can only remove carbon, nitrogen, sulphur and oxygen. It cannot remove nickel or molybdenum economically, so every kilogram of those elements has to be bought in the charge.
Typical charge components for an 18-8 austenitic heat are clean 304 process scrap and returns, purchased 304 or 316 scrap sorted by alloy family, low-carbon carbon steel scrap used as a diluent to hit the carbon and nitrogen targets, high carbon ferrochrome as the main chromium carrier, ferronickel or pure nickel cathode for the nickel balance, ferromolybdenum for molybdenum-bearing grades, plus ferromanganese, ferrosilicon and aluminium for deoxidation and alloy trimming. Scrap must be free of copper, lead, zinc, tin and brazing alloys, because copper and tin cannot be oxidized out and remain in the steel, raising hot shortness and lowering hot ductility during casting and rolling.
Sorting discipline is therefore a raw material property in its own right. Hand-held X-ray fluorescence sorting of incoming scrap, plus a ban on mixed turnings and on material from shredders handling electronic scrap, is what keeps residual copper below the 0.30% to 0.50% levels that most austenitic plate specifications tolerate. A heat that arrives at the caster with 0.6% Cu and 0.05% Sn will show edge cracking in the roughing passes no matter how the reheating furnace is tuned.
Chemistry Window That Defines the Delivered Grade
The purchased plate is accepted against a product standard, not against the mill's internal aim. For hot rolled stainless plate the reference documents are ASTM A240/A240M, GB/T 4237, JIS G 4304 and EN 10088-2, and the chemistry of the most common medium plate grades falls in the windows below. A mill that lands a 304 heat at 17.6% Cr because it leaned on stainless scrap with a low chromium yield has produced a heat that can still be called 304 on a certificate, but leaves no margin for the chromium-depleted zone that forms beside grain boundaries during welding.
| Grade (UNS) | C max % | Cr % | Ni % | Mo % | Other required | Typical plate duty |
|---|---|---|---|---|---|---|
| 304 (S30400) | 0.08 | 18.0-20.0 | 8.0-10.5 | - | Mn 2.00 max, Si 0.75 max, P 0.045 max, S 0.030 max | General tanks, structural covers, 3-20 mm |
| 304L (S30403) | 0.030 | 18.0-20.0 | 8.0-12.0 | - | N 0.10 max | Welded vessels without post-weld anneal |
| 316L (S31603) | 0.030 | 16.0-18.0 | 10.0-14.0 | 2.00-3.00 | N 0.10 max | Chloride-bearing process streams, 6-25 mm |
| 321 (S32100) | 0.08 | 17.0-19.0 | 9.0-12.0 | - | Ti 5x(C+N) min, 0.70 max | Elevated temperature service, 400-800 C |
| 310S (S31008) | 0.08 | 24.0-26.0 | 19.0-22.0 | - | Mn 2.00 max, Si 1.50 max | Furnace parts, radiant sections, above 900 C |
Two chemistry points matter more than buyers expect. First, nitrogen: a deliberate 0.05% to 0.10% nitrogen addition raises annealed strength without hurting ductility, but uncontrolled nitrogen pick-up during argon oxygen decarburization produces internal porosity in the slab that only appears after the plate is machined. Second, carbon in 316L and 304L: the 0.030% limit is not a metallurgical nicety. At 0.030% C a 10 mm plate can be welded and cooled through the 425 C to 815 C sensitization range without chromium carbide precipitation reaching a level that fails an intergranular corrosion test, which is precisely why the low-carbon variant is specified for vessel work.
Cast Slab Quality and the Defects That Follow It Into the Plate
Continuous casting an austenitic stainless slab is a heat-transfer problem before it is a metallurgical one. If secondary cooling is uneven, the slab leaves the caster with a deep oscillation mark structure, transverse corner cracks, or a centreline segregation band enriched in chromium and molybdenum. Those defects are not removed by reheating; they are inherited. Transverse corner cracks open further during roughing and have to be ground out, generating extra scarfing and a shorter usable slab. Centreline segregation survives rolling as a band with a different corrosion potential, which is why heavy plate cut from the centre of a poorly cast slab can pit preferentially along the mid-thickness plane.
Accepted practice is to scarf or grind slab surfaces to remove casting skin and corner defects before reheating, to hold a controlled electromagnetic stirring regime during solidification, and to verify slab quality by visual and ultrasonic inspection on grades intended for pressure service. Slab thickness choice is a compromise: a thicker 220 mm slab gives more reduction to a 6 mm plate, which refines the cast structure, but requires a bigger reduction schedule and a heavier mill. A rule of thumb used in plate plants is to keep total reduction from slab to finished plate above about 6:1 for critical service and above 3:1 for general structural work.
Reheating and Hot Rolling Windows
Slabs are reheated to 1200 C to 1280 C for the 300 series, held long enough to dissolve any residual carbides and equalize temperature through the thickness, then descaled with high pressure water at roughly 180 to 200 bar before the first roughing pass. Overheating is a real risk: above about 1300 C the delta ferrite content rises sharply and the slab becomes prone to edge tearing during roughing, while an under-soaked slab rolls with a hard core that produces thickness deviation and residual stress in the delivered plate.
Finish rolling temperature for austenitic plate is normally kept above 900 C to avoid strain-induced martensite and to leave the structure fully austenitic. After rolling, the plate is either air cooled or, for grades where carbide precipitation must be suppressed, water quenched from above 1000 C. That cooling practice, not the rolling itself, decides whether the plate will pass an intergranular corrosion test on delivery. Ferritic grades such as 430 need a different thermal route entirely, with lower reheating temperatures and annealing around 800 C to 850 C, and they are far more sensitive to grain coarsening and to the 475 C embrittlement range.
Coil, Cut Length or Plate: Which Feedstock the Order Actually Needs
The upstream article this page replaces described hot rolled coil as the raw material for plate, which is only partly true. There are three distinct feedstock routes and they are not interchangeable for a given purchase order.
| Feedstock | Thickness capability | Finish on delivery | Where it is the right choice | Where it fails |
|---|---|---|---|---|
| Continuous cast slab, plate mill | 6-60 mm and above | No.1 hot rolled annealed and pickled | Heavy plate, pressure parts, thick flanges, wide widths | Uneconomic below 6 mm in most mills |
| Hot rolled coil, cut to length | 2-12 mm | No.1, optionally levelled and edge trimmed | Medium plate in coil-fed lines, long runs of one width | Coil set and crossbow after cutting if levelling is weak |
| Cold rolled hard coil | 0.3-3 mm | 2D, 2B or hard temper as rolled | Thin sheet, tube feedstock, further cold reduction | Cannot deliver 6 mm and thicker; hardness blocks forming |
When a hot rolled coil is decoiled and cross-cut, the plate inherits the coil's internal stress pattern. Without a tension leveller or a roller leveller with sufficient backup roll support, 6 mm to 10 mm cut lengths come out with edge wave or centre buckle that only shows up after laser cutting, and the flatness measured on the mill floor looks acceptable because the plate is still restrained by its own weight. Flatness requirements should be written into the order with a measurable limit, such as 5 mm per metre for 6 mm plate, rather than phrased as good flatness.
Cold Rolled Hard Coil as a Feedstock and Its Hardness Ceiling
Pickled hot rolled coil that is subsequently cold rolled becomes a hard temper product because cold reduction stores dislocations in the austenite, and austenitic stainless steel work hardens faster than almost any other common metal: a 40% to 60% reduction can take Type 304 from roughly 200 HV to well over 350 HV. Hardness above 90 HRB is normal for hard rolled 304, tensile strength climbs into the 1000 MPa class, and elongation in 50 mm falls to single digits. ASTM A666 defines the temper range for cold rolled austenitic flat products, running from annealed through quarter hard, half hard, full hard, with minimum tensile strength rising from about 860 MPa at half hard to about 1275 MPa at full hard for Type 304.
The practical consequence for a buyer is that hard coil is a legitimate feedstock for tube mills, for hot dip coating lines that have their own in-line annealing furnace, and for parts that only need a single bend of less than 90 degrees perpendicular to the rolling direction, but it is not a substitute for hot rolled plate. A hard coil cannot be sheared into 10 mm structural plate because it is not 10 mm thick, and it cannot be formed into a dished head because the stored strain leaves almost no residual ductility. Orders that specify cold rolled material for a part that will be deep drawn or rolled to a radius will fail at the fabricator, not at the mill.
Annealing and Pickling: Turning a Rolled Surface Into a Deliverable One
Hot rolled plate leaves the mill covered in a mill scale of mixed chromium and iron oxides that is not protective and must be removed before the plate can develop its passive film. Two routes exist. Continuous annealing and pickling lines process coil at speed through a furnace at 1050 C to 1120 C for austenitic grades followed by water quenching, then through electrolytic sodium sulphate descaling and a mixed nitric-hydrofluoric acid pickle, then a final passivation rinse. Batch annealing followed by a separate pickling line is used for plate that cannot run through a coil line; the risk there is slower, less uniform heating and a heavier scale that needs longer acid exposure, which increases the chance of over-pickling and a roughened surface.
The delivered finish should be stated by its standard designation rather than by description: No.1 for hot rolled annealed and pickled plate, 2D for cold rolled annealed and pickled, 2B for cold rolled annealed and skin passed, with No.4 polished and BA bright annealed available on thinner material. ASTM A480/A480M defines these finishes together with the thickness and flatness tolerances for flat rolled stainless, and EN 10029 covers dimensional tolerances for hot rolled plate in the 3 mm to 400 mm range. Quoting a plate as pickled without naming the standard finish leaves the surface roughness, the residual scale at the edges and the permissible surface defects undefined.
Receiving Inspection: What to Check on Incoming Slab, Coil and Plate
Incoming material control should be proportional to the risk in the end use. For any plate destined for pressure or cryogenic service, the minimum package is a certificate of analysis traceable to the heat number, a check of the heat number stamped or stencilled on the plate against that certificate, PMI verification of chromium, nickel and molybdenum on at least one point per plate, dimensional check of thickness at several points across the width, and a visual examination for rolled-in scale, slivers, seams and edge laminations.
Thickness deserves special attention because it is where feedstock economics quietly transfer risk. A plate rolled from a coil that was at the bottom of its tolerance, then descaled and pickled, then levelled, can finish at 3% to 5% below nominal and still be inside a wide tolerance class. Where the plate is a pressure boundary, order to a restricted thickness tolerance class and measure with a calibrated ultrasonic thickness gauge rather than a micrometer at the edge only. For plate above 20 mm, add ultrasonic inspection to a defined acceptance level for laminations, since a centreline defect inherited from the slab cannot be seen from either surface.
Finally, record the mill's heat number on the goods receiving document and keep the cut-off end of the plate. If a corrosion or cracking problem appears after fabrication, the retained sample is what allows a metallurgical investigation to distinguish a raw material defect from a fabrication error.
Cost Structure of the Raw Material Chain
Plate price is driven less by rolling cost than by the metallic charge, and the charge is dominated by nickel and molybdenum units. A 316L heat carries roughly 2.5% molybdenum and 12% nickel against 8% nickel and no molybdenum in 304, which is why the two grades separate in price by far more than their weight difference suggests. Buyers comparing offers should normalize on chemistry actually delivered, not on grade name: a 316L certified at 16.2% Cr and 2.1% Mo is a different commercial object from one at 17.5% Cr and 2.9% Mo, even though both meet the same specification window. Asking for the certificate of analysis before comparing prices is the only way to keep the comparison honest, and it costs nothing.
FAQ
Q: What is the primary raw material for hot rolled stainless steel medium plate?
The primary feedstock is a continuously cast stainless slab of about 180 mm to 220 mm thickness, produced from a charge of sorted stainless scrap, high carbon ferrochrome, ferronickel or nickel, and ferromolybdenum, melted in an electric arc furnace and refined in an argon oxygen decarburization vessel.
Q: Can hot rolled stainless plate be produced from cold rolled hard coil?
No. Cold rolled hard coil is 0.3 mm to 3 mm thick and work hardened to above 90 HRB, so it cannot supply a 6 mm to 20 mm plate, and its low residual ductility rules out forming operations such as dishing or rolling to a small radius.
Q: Why is copper limited in the scrap charge for stainless steel?
Copper and tin cannot be removed by argon oxygen decarburization or vacuum treatment, so they accumulate in the heat; above roughly 0.30% to 0.50% Cu the steel becomes hot short and shows edge cracking during roughing and transverse cracking during casting.
Q: What slab to plate reduction ratio should be specified?
A total reduction above about 6:1 is normal for pressure and critical service plate, and above 3:1 for general structural plate, because reduction is what converts the coarse cast dendritic structure into a wrought, homogeneous one.
Q: What is the difference between No.1 and 2B finish on stainless plate?
No.1 is hot rolled, annealed and pickled, with a matte grey surface and a roughness suitable for further grinding or for structural work; 2B is cold rolled, annealed and skin passed, giving a smoother, brighter surface on thinner material, and is defined in ASTM A480/A480M.
Q: Is hot rolled coil simply cut into plate?
Only in coil-fed cut-to-length lines for 2 mm to 12 mm material. Plate above that thickness is rolled from slab in a plate mill, and cut lengths from coil need tension or roller levelling to avoid edge wave and centre buckle after cutting.