In the past 30 years, Inconel 690 alloy wear-resistant steel plate has been gradually replaced by Inconel 600 alloy wear-resistant steel plate in order to improve the reliability of steam generator heat exchange tubes in nuclear power plants and avoid leakage due to early stress corrosion. The heat treatment of Inconel 690 alloy wear-resistant steel plate is generally solid solution treatment + special heat treatment (TT treatment), in the process of production and use, the material is distributed along the grain boundaries or precipitated carbide. Some data show that chromium deficiency near the grain boundary will be caused during the process of carbide precipitation along the grain boundary, especially Cr23C6, when the chromium content is below a certain value, intergranular corrosion and stress corrosion will be caused. In this paper, the size, morphology and distribution characteristics of grain boundary precipitates of Inconel 690 alloy wear-resistant steel plate after solution and TT treatment at different temperature and time were studied.

The sample material is produced and smelted by vacuum induction + electroslag remelting process. After extrusion, cold drawing and cold rolling, the sample material is Φ19.05mm×1.09mm. Its main chemical composition (mass fraction, %) is: 0.22Mn, 0.02C, 0.06Si, 9.48Fe, 60.10Ni, 29.51Cr, 0.30Ti, 0.27Al, 0.002S, 0.005P, etc. The cold rolled Inconel 690 alloy wear-resistant steel plate was treated by solution treatment and TT treatment at different temperatures, the solution treatment temperatures were 950, 1000, 1050, 1100 and 1150℃, held for 5min, and water cooled. TT treatment processes are 600℃×12h, 700℃×12h, 700℃×24h, 700℃×48h, 700℃×96h, 800℃×12h, 800℃×24h, 800℃×48h, and the cooling method is water cooling.

The microstructure of Inconel 690 alloy wear-resistant steel plate after solution treatment is austenite + a small amount of carbide + a small amount of Ti(C, N). When the solution temperature is lower than 1100℃, the grain size changes little, and when the solution temperature exceeds 1150℃, the grain size increases rapidly. Therefore, the solution treatment temperature of wear-resistant steel plate is recommended below 1100℃. The grain boundary particles are mainly Ti(C, N) and M23C6 precipitated along the grain boundary, and their quantity and size increase with the increase of TT treatment temperature and the extension of holding time, mainly in intermittent and semi-continuous distribution.