Apr 03, 2024 Leave a message

Shipbuilding Steel Plate Processing by Grade: From A to FH36 — Rolling, Cutting, Welding and Certification

Shipbuilding steel plates are not one product - they form a graded family where the letter in the grade name determines the rolling process, the allowable cutting and welding procedures, and ultimately which part of the ship the plate can go into. General-strength grades A, B, D and E serve hull structures that do not carry primary stress. High-strength grades AH36, DH36, EH36 and FH36 - with their 355 MPa minimum yield - go into decks, bottom shells and critical stiffeners. This guide explains what changes from one grade to the next in processing terms and what shipyards and fabricators must check before the first cut.

 

Shipbuilding steel plates

Key Takeaways

  • Grade A & B - the simplest production route: conventional hot rolling. Suitable for inland and coastal vessels, non-critical structures.
  • Grade D & E - require controlled rolling or normalising to meet -20°C and -40°C impact requirements. Used in ocean-going hulls exposed to cold water.
  • AH36 / DH36 / EH36 / FH36 - high-strength grades (YS ≥355 MPa). DH36 and above typically need TMCP (thermo-mechanical controlled processing) or normalising. FH36, with a -60°C Charpy requirement, demands the most rigorous processing.
  • Welding consumables and procedures must match the grade. Using an E6013 rod on EH36 plate will fail classification society survey.
  • All hull plates must carry a classification society stamp (ABS, LR, DNV, BV, CCS, etc.) on the Mill Test Certificate. Without it, the plate cannot legally go into a classed vessel.

1. The Grade Family at a Glance

 

Shipbuilding steel falls into two strength categories: general-strength (often called "normal-strength" in some class rules) and high-strength. The table below shows the complete picture.

Category Grades Min. Yield Strength (MPa) Tensile Strength (MPa) Impact Test Temp (°C) Typical Thickness (mm)
General Strength A 235 400–520 N/A (no impact test) 6–150
General Strength B 235 400–520 0 6–150
General Strength D 235 400–520 -20 6–150
General Strength E 235 400–520 -40 6–150
High Strength (32 ksi) AH32, DH32, EH32, FH32 315 440–570 0 / -20 / -40 / -60 6–100
High Strength (36 ksi) AH36, DH36, EH36, FH36 355 490–620 0 / -20 / -40 / -60 6–100
High Strength (40 ksi) AH40, DH40, EH40, FH40 390 510–650 0 / -20 / -40 / -60 6–100

Source: ABS Rules for Materials and Welding, Part 2; IACS UR W11 (normal and higher-strength hull structural steels). Values are for thickness ≤50 mm; thicker sections may have adjusted minima. Minimum impact energy: 27 J at the specified temperature for general-strength grades; typically 34 J for high-strength (class-dependent).

 

2. Processing Route by Grade - Why D and E Cost More Than A

 

Grade A and B: Conventional Hot Rolling

Grade A and B plates are produced by straightforward hot rolling: reheat the slab to ~1200°C, roll to finished thickness, air-cool. No controlled cooling, no normalising. The as-rolled ferrite/pearlite microstructure delivers adequate strength and ductility for inland vessels, barges and non-critical structural members. Processing cost is the lowest in the ship plate family. Cutting and welding are similarly simple - oxy-fuel or plasma cutting with standard shop practice, manual arc welding with E6013 or E7018 electrodes, no mandatory preheat below 30 mm thickness.

 

Grade B adds one step: a Charpy V-notch impact test at 0°C. The chemistry must keep phosphorus and sulphur low enough (≤0.035% each) to avoid embrittlement, but the rolling process is unchanged from Grade A.

 

Grade D: Normalised or Controlled-Rolled

Grade D must meet a -20°C impact requirement. That forces a finer grain size than as-rolled processing can deliver. Two production routes are accepted:

  • Normalising: reheat the rolled plate to 890–920°C, hold, air-cool. This refines the grain structure and improves toughness uniformity. Adds roughly 10–15% to the production cost versus as-rolled.
  • Controlled rolling (TMCP without accelerated cooling): lower the finishing temperature to 780–830°C so that austenite recrystallises into fine grains. This is less expensive than normalising but requires tight temperature control and higher mill loads.

 

Grade E and All EH/FH High-Strength Grades: The Full TMCP Route

Grade E (-40°C impact) and the high-strength EH/FH grades (-40°C and -60°C) need the highest level of grain refinement. The standard production route is TMCP (thermo-mechanical controlled processing) with accelerated cooling:

 

  • Controlled roughing: heavy reduction passes above the recrystallisation temperature to break up the as-cast grain structure.
  • Controlled finishing: lower-temperature passes in the non-recrystallisation region (typically 850–780°C) to elongate and pancake the austenite grains, creating a high density of nucleation sites.
  • Accelerated cooling: water cooling at 5–30°C/s to transform the deformed austenite into fine-grained ferrite with dispersed pearlite or bainite.

 

The result is a grain size of ASTM 8–10 (10–20 μm), which gives both the 355 MPa yield strength and the -40°C or -60°C toughness. This process requires a modern plate mill with powerful descaling, precise temperature measurement and a multi-zone accelerated cooling system. It adds 20–30% to the baseline rolling cost.

 

Grade Production Route Relative Cost Typical Applications
A, B Conventional hot rolling 1.0× Inland vessels, barge hulls, non-critical stiffeners
D Normalised or controlled-rolled 1.10–1.15× Ocean-going hulls, decks, bulkheads
E TMCP with accelerated cooling 1.20–1.30× Ice-class vessels, Arctic service, LPG/LNG tanks
AH36, DH36 TMCP or normalised 1.15–1.25× Primary hull structure, bottom shell, strength deck
EH36, FH36 TMCP with accelerated cooling 1.25–1.40× Arctic hulls, high-stress zones, jack-up rig legs

Cost multipliers are indicative. Actual pricing depends on plate dimensions, quantity and market conditions.

 

3. Cutting and Edge Preparation

 

Shipbuilding plate cutting is dominated by three processes: oxy-fuel, plasma and water-jet. The choice depends on thickness and grade.

  • Oxy-fuel (flame cutting): standard for plates 10–150 mm. Clean cut, low equipment cost. Preheating before cutting is required for EH36 and FH36 above 30 mm, and for all grades above 50 mm, to avoid hardening cracks at the cut edge.
  • Plasma cutting: faster than oxy-fuel for plates below 25 mm. Produces a narrower heat-affected zone (HAZ). Preferred for AH36/DH36 where minimum HAZ hardening is desired.
  • Water-jet cutting: cold process, zero HAZ. Used for FH36 and EH36 where edge cracking risk must be eliminated. Slower and more expensive - reserved for critical-profile parts.

 

After cutting, edges must be ground smooth to remove slag and any micro-cracks. For primary hull members, classification societies often require the cut edge to be inspected by magnetic particle testing (MT) or dye penetrant (PT).

 

4. Welding Procedures - Match the Consumable to the Grade

 

Welding is where most shipyard non-conformances occur on higher grades. The table below gives the general consumable selection for shielded metal arc welding (SMAW), which remains the most common method in ship assembly.

Plate Grade Recommended SMAW Electrode (AWS) Preheat (≥25 mm thickness) Max. Interpass Temp.
A, B E6013, E7018 None below 30 mm; 50°C above 250°C
D, E E7018, E7018-1 None below 25 mm; 75°C above 200°C
AH36, DH36 E7018-1, E8018-C3 100°C (all thicknesses) 200°C
EH36 E8018-C3, E9018-M 125°C (all thicknesses) 180°C
FH36 E9018-M, E11018-M 150°C (all thicknesses) 150°C

 

Three welding rules that apply across all shipbuilding grades:

  • Low-hydrogen practice is mandatory for EH36 and above. Electrodes must be baked at 350–400°C for 1–2 hours and stored in a holding oven at 120°C. A wet electrode on FH36 can cause hydrogen-induced cracking visible only days after welding.
  • Heat input must be controlled. Above 4.0 kJ/mm, the HAZ grain coarsens and toughness drops. Below 1.0 kJ/mm, the cooling rate is too fast and hard phases (martensite) can form. A typical target for EH36/FH36 is 1.5–3.0 kJ/mm.
  • Tack welds count. Tack welds on EH36 and FH36 must use the same low-hydrogen consumables and preheat as the main weld. Small, fast tacks with the wrong electrode are a common cause of cracking found later during UT inspection.

 

5. Cold Forming and Bending - What the Grade Letter Tells You

 

Ship hull plates are rarely used flat. They are rolled into shell curvature, pressed into stiffener profiles, and bent into brackets. Cold forming is the standard method, but the minimum bend radius depends on the grade and the rolling direction.

Grade Min. Bend Radius (t = plate thickness) Remarks
A, B 1.0 t No restrictions for bends transverse to rolling direction
D, E 1.5 t Transverse bending preferred; parallel to rolling direction needs 2.0 t
AH36, DH36 2.0 t Higher springback than general-strength grades; overbend by 3–5°
EH36, FH36 2.5 t (t ≤ 25 mm); 3.0 t (t > 25 mm) Warm forming (150–200°C) recommended for tight radii to avoid cracking

 

These are shop-floor guidelines. The shipyard's approved forming procedure, qualified to the class society's satisfaction, takes precedence.

A practical note: the higher-strength grades spring back more after cold forming. A DH36 plate bent to a 90° angle will relax to roughly 87° when the press is released. Shipyards compensate by overbending; the amount is determined by trial on the first piece.

 

6. Classification Society Certification - The Gatekeeper

 

No shipbuilding plate enters a classed vessel without the stamp of a recognised classification society. The major societies relevant to Chinese steel exports are:

  • ABS - American Bureau of Shipping (Houston)
  • LR - Lloyd's Register (London)
  • DNV - Det Norske Veritas (Oslo)
  • BV - Bureau Veritas (Paris)
  • CCS - China Classification Society (Beijing)
  • RINA - Registro Italiano Navale (Genoa)
  • ClassNK - Nippon Kaiji Kyokai (Tokyo)
  • KR - Korean Register (Busan)

 

Each society publishes its own "Rules for Materials and Welding," but all comply with the IACS (International Association of Classification Societies) Unified Requirements. A steel mill must undergo an initial audit by each society whose stamp it wishes to use, followed by annual surveillance audits and periodic re-certification. The surveyor witnesses the mechanical testing and stamps each Mill Test Certificate (EN 10204 3.1 or 3.2).

 

For the buyer, this means: check the certificate before accepting the plates. A plate without a valid class stamp cannot be used in a classed vessel, period. If your order specifies "ABS Grade AH36," every plate must arrive with an ABS-stamped MTC showing the heat number, chemical composition, tensile results, impact results and the surveyor's signature.

 

7. Grade Selection Guide - Which Plate for Which Part of the Ship?

 

Ship Area Typical Grade Reason
Main deck (strength deck) AH36, DH36 High longitudinal stress; 355 MPa yield needed
Bottom shell plating AH36, DH36, EH36 (ice belt) Hydrostatic pressure + wave bending; ice belt needs -40°C toughness
Side shell (above waterline) A, B, AH32, AH36 Lower stress zone; grade A sufficient for tropical/ temperate service
Bulkheads (transverse & longitudinal) A, D Non-primary structure; general strength sufficient
Hatch coamings & covers AH36, DH36 High local loads from cargo + green water
LNG / LPG tank shells E, EH36, FH36 Cryogenic service; -60°C toughness mandatory
Jack-up rig legs & spudcans EH36, FH36, EQ47, EQ56 Extreme cyclic loading + cold water; highest-grade plates used
Superstructure (accommodation block) A Low stress; cost-driven selection

 

Frequently Asked Questions

 

What is the difference between Grade A, B, D and E shipbuilding steel plates?

Grades A, B, D and E are general-strength hull structural steels with minimum yield strength of 235 MPa. The key difference is low-temperature impact toughness: Grade A requires no impact testing; Grade B is tested at 0°C; Grade D at -20°C; Grade E at -40°C. Higher-letter grades are specified for colder service environments, particularly for ice-class vessels and Arctic operations.

 

Why do AH36, DH36, EH36 and FH36 require different rolling processes?

These high-strength grades (minimum yield 355 MPa) demand both higher strength and low-temperature toughness - a combination that requires precise grain refinement. AH36 and DH36 can often be produced by controlled rolling (TMCP) alone. EH36 typically requires normalizing or TMCP with accelerated cooling. FH36, with a -60°C impact requirement, needs the most stringent process: low finishing temperature, rapid cooling and sometimes normalizing heat treatment.

 

What welding precautions are needed for EH36 and FH36 shipbuilding plates?

EH36 and FH36 require:

(1) low-hydrogen welding consumables (AWS E8018-C3 or E9018-M);

(2) preheat to 100–150°C for thicknesses above 25 mm;

(3) controlled heat input (typically 1.5–3.5 kJ/mm);

(4) interpass temperature kept below 200°C;

(5) post-weld inspection by ultrasonic testing (UT) or radiographic testing (RT) as required by the classification society. WPS must be qualified per IACS UR W28.

 

Do shipbuilding steel plates need classification society certification?

Yes. All hull structural steel plates must be certified by a recognised classification society such as ABS, LR, DNV, BV, CCS, RINA, ClassNK or KR. The mill must hold valid approval from each society whose stamps appear on the material. Plates are shipped with Mill Test Certificates (EN 10204 3.1 or 3.2) bearing the class society stamp and surveyor signature.

 

What shipbuilding grades does Gnee Steel supply?

Gnee Steel (Tianjin) Co., Ltd. supplies Grade A, B, D, E and high-strength AH32, DH32, EH32, AH36, DH36, EH36 and FH36 in thicknesses from 6 mm to 150 mm, certified to ABS, LR, DNV, BV, CCS, RINA and other major classification societies. We also offer cutting, edge preparation and prime coating. Contact our team for a quotation with your required grade, dimensions and certification requirements.

 

References

ABS. Rules for Materials and Welding, Part 2. American Bureau of Shipping.

IACS. UR W11 - Normal and Higher Strength Hull Structural Steels. International Association of Classification Societies.

IACS. UR W28 - Welding Procedure Qualification for Hull Structural Steels.

Kloeckner Metals. ABS A131 AH36, DH36, EH36, FH36 Steel Plate. 

Octal Metals. AH36, DH36, EH36 High Strength Shipbuilding Steel Plate. 

GB/T 712-2022 - Structural Steel for Ships and Offshore Structures. China National Standard.

Gnee Steel product catalogue - shipbuilding steel plates. 

 

Need Shipbuilding Steel Plate - ABS, LR, DNV or CCS Certified?

Gnee Steel supplies Grade A through FH36 with full class society certification. Send your spec (grade, dimensions, class society, quantity) and get a quotation within 24 hours.

Get a Quote

 

Or email info@gneesteels.com · WhatsApp +86 15824687445 ·

 

GNEE has provided a wide variety of well-established steel service centers and end-users in the ocean engineering sector with reliable steel products for over a decade. We have established long-term cooperative relations with hundreds of mills to ensure these products are fabricated using premium material and are in sync with various international standards.

China shipbuilding steel plate manufacturer

 

Disclaimer: This article is provided for general technical information and does not constitute engineering advice or a substitute for approved Welding Procedure Specifications. Always follow the applicable classification society rules and your shipyard's qualified procedures. Gnee Steel (Tianjin) Co., Ltd. No.4-1114, Beichen Building, Beicang Town, Beichen District, Tianjin, China. All Rights Reserved.

Send Inquiry

whatsapp

phone

Email

Inquiry