Mar 12, 2024NM400 Wear Plate: How Cooling Rate Sets Structure and HardnessNM400 is a 400 HBW abrasion-resistant plate whose hardness is created by the cooling path after the last rolling pass, not by carbon content alone. This article explains the contin -
Mar 12, 2024AOD Melting Improvements for Crack-Free Wear-Resistant PlateCracking in wear-resistant plate usually starts in the melting shop, not the heat-treatment furnace. This article explains how AOD refining balances decarburization against chromiu -
Mar 12, 2024700 °C Long-Term Aging of Alloy 282: Carbides and ToughnessAlloy 282, UNS N07282, is a candidate material for 700 °C advanced ultra-supercritical boiler components. This article follows its microstructure and mechanical properties through -
Mar 11, 202418Cr2Ni4WA Carburizing Steel: Heat Treatment and Case Control18Cr2Ni4WA is a 4% nickel-chromium-tungsten case-hardening steel from GB/T 3077, chosen for heavy sections that need a 58-62 HRC case over a tough core. This guide covers its compo -
Mar 11, 202420MnCr5 (1.7147) Case-Hardening Steel: Heat Treatment Guide20MnCr5 (1.7147) is a manganese-chromium carburising steel to EN 10084, widely used for gearbox shafts and gears in the 10-60 mm section range. This article sets out its compositio -
Mar 11, 2024S30432 Austenitic Steel: Structure After 650C Stress AgingS30432 is a copper-, niobium- and nitrogen-bearing 18Cr-9Ni austenitic steel for ultra-supercritical boiler superheater and reheater tubes, not a wear-resistant plate. Long-term ag -
Mar 11, 202420Cr2Ni4A Heat Treatment: Temperature, Soaking and Case Depth20Cr2Ni4A is a high-nickel carburising steel to GB/T 3077 used for heavy gears, shafts and bearing rings where a hard case must sit on a tough core. Its treatment involves five dis -
Mar 11, 202420Cr3MoWVA High-Temperature Bolt Steel: Data and Heat Treatment20Cr3MoWVA is a 3% Cr-Mo-W-V alloy steel used for bolted joints running at 500-570 C, where loss of clamp load rather than fracture is the design concern. The article sets out its -
Mar 11, 2024Annealing Treatment of Alloy Wear-Resistant Plate: Structure and Property Res...This study compares two-phase zone, single-phase zone and double annealing of an alloy wear-resistant plate bar with a phase transformation point of 845 ± 5 °C. It reports how each -
Mar 11, 2024Selecting Stainless Steel for Corrosive EnvironmentsStainless steel selection should start from the service conditions and the governing corrosion mechanism rather than from a familiar grade. The article covers corrosion-rate classe -
Mar 11, 2024Sub-Temperature Quenching and Impact Toughness of 30CrMnSi PlateQuenching 30CrMnSi wear plate from the intercritical band rather than above Ac3 refines the martensite and leaves isolated ferrite islands, which raises impact energy at a given ha -
Mar 11, 202420CrMnTi Carburizing Steel Plate: Composition and Case Hardening20CrMnTi is a low-carbon Cr-Mn-Ti carburizing steel to GB/T 3077, supplied as plate for gear blank and wear part production. The article sets out its composition limits, core mecha